Polymer Property : Vicat Softening Point = 180 °C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Vicat Softening Point 180 °C
356 °F
ISO 306
Radici Radiflam® BN100 AE Polybutylene Terephthalate
PBT Self-extinguishing with halogenInformation provided by Radici group.
Vicat Softening Point 180 °C

@Load 5.10 kg
356 °F

@Load 11.2 lb
50°C/h
Radici Radilon® A USZ200 (dry) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Vicat Softening Point 180 °C
356 °F
49 N; ISO 306, ASTM D1525
Nilit Nilamid B3 H ZB Unfilled, Low Temperature Impact Resistant PA6
Description: Nilamid B3 H ZB is a high impact NYLON 6. The product has excellent impact properties, even at minus temperatures, whilst maintaining mechanical characteristics. Application areas inclu..
Vicat Softening Point 180 °C
356 °F
50°C/h 50N; ISO 306
LATI LATILUB 95-25GR CE/10 Polysulfone Base (PSU), 25% Graphite, 10% Special Mineral Filled Self Lubricating Plastic
Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri..
Vicat Softening Point 180 °C
356 °F
50°C/h 50N; ISO 306
LATI LASULF Polysulfone (PSU)  (Unverified Data**)
Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi..
Vicat Softening Point 180 °C
356 °F
50°C/h 50N; ISO 306
Lanxess Durethan® BC 40 SR2 000000 Nylon 6
PA 6 injection molding grade, high viscosity, non-reinforced, higher notched impact strength than BC 30, impact-modified
Vicat Softening Point 180 °C
356 °F
50°C/h 50N; ISO 306
Lanxess Pocan® B 1305 000000 PBT
PBT, non-reinforced, injection molding
Vicat Softening Point 180 °C

@Load 5.00 kg
356 °F

@Load 11.0 lb
LATI Latamid 12 G/50 PA 12, 50% Glass Fiber Reinforced
Polyamide 12 (PA12) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Vicat Softening Point 180 °C

@Load 5.00 kg
356 °F

@Load 11.0 lb
LATI Latamid 66 H2PX-V0 PA 66, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin ..
Vicat Softening Point 180 °C
356 °F
50°C/h 50N; ISO 306
Lanxess Pocan® DP 1105 000000 PBT
PBT, non-reinforced, injection molding, extrusion, improved flowability
Vicat Softening Point 180 °C

@Load 5.00 kg
356 °F

@Load 11.0 lb
LATI Latishield 75/4-10A PBT, Steel Fiber Reinforced
EMI shielding product based on Polybutylene Terephthalate (PBT). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu..
Vicat Softening Point 180 °C
356 °F
Rate A/50; ISO 306
SABIC Innovative Plastics Ultem ATX100R PEI (Europe-Africa-Middle East)
Higher impact, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 HB Listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Vicat Softening Point >= 180 °C
>= 356 °F
ISO 306
Solvay Specialty Polymers Ryton® QA200P Polyphenylene Sulfide (PPS)
Ryton® QA200P (pelletized) unfilled polyphenylene sulfide exhibits excellent thermal stability and chemical resistance and may be used in injection molding processes.Features: Good Chemical Resis..
Vicat Softening Point 180 °C
356 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Valox® EH7020HF PBT+PET (Asia Pacific)
Valox EH7020HF is a mineral filled PBT/PET that offers good surface appearance, high flow and good heat performance. EH7020HF was developped for automotiove bezel application that require basecoat +..
Vicat Softening Point 180 °C
356 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Valox® EH7020HF PBT+PET (Asia Pacific)
Valox EH7020HF is a mineral filled PBT/PET that offers good surface appearance, high flow and good heat performance. EH7020HF was developped for automotiove bezel application that require basecoat +..
Vicat Softening Point 180 °C
356 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Valox® VIC4311 PBT
VALOX VIC4311 is a 30% glass filled, impact modified PBT with excellent epoxy adhesion. Automotive underhood applications such as ignition coil housings.
Vicat Softening Point 180 °C
356 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Xenoy® 6380U PBT+PET (Asia Pacific)
XENOY 6380U is a 30% glass reinforced, UV stabilized grade, that combines high stiffness with improved ductility. The combination of mechanical properties at high and low temperatures and chemical r..
Vicat Softening Point 180 °C
356 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Xenoy® 6380U PBT+PET (Asia Pacific)
XENOY 6380U is a 30% glass reinforced, UV stabilized grade, that combines high stiffness with improved ductility. The combination of mechanical properties at high and low temperatures and chemical r..
Vicat Softening Point 180 °C
356 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA
NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin..
Vicat Softening Point 180 °C
356 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA
NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity..
Vicat Softening Point 180 °C
356 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA (Europe-Africa-Middle East)
NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity..
Vicat Softening Point 180 °C
356 °F
Rate B/120; ISO 306
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS
Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl ..
Vicat Softening Point 180 °C
356 °F
ASTM D1525
Goodfellow TPX® DX231 Coating/Extrusion Grade Polymethylpentene
This grade is highly recommended for paper coating or for fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release characteristics a..
Vicat Softening Point 180 °C
356 °F
50N; ISO 306
Eurotec® Tecodur® PB70 NL XA 20 PBT unreinforced, UL94 V0
Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance..
Vicat Softening Point 180 °C
356 °F
B/120; ISO 306
Eurostar Staramide BST03 PA6, Impact Modified, Injection Molded
BST03 is an Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Vicat Softening Point 180 °C
356 °F
Rate B/50; ASTM D 1525
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Asia Pacific)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Asia Pacif..
Vicat Softening Point 180 °C

@Load 5.00 kg
356 °F

@Load 11.0 lb
LATI Latilub 95-25GR CE/10 PSU, Mineral Fiber Reinforced, Graphite Filled
Self-lubricating product based on Polysulfone (PSU). Graphite. Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu..