| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Mineral Reinforced |
| Manufacturer | Polykemi AB |
| Trade Name | POLYfill |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Polykemi AB POLYfill PPC B10075 Polypropylene Copolymer, Mineral Reinforced.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 2.25 g/cc | 0.0813 lb/in³ | ISO 1183 |
| Filler Content | 75 % | 75 % | ±2%; Polykemi |
| Melt Index of Compound | 10 g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C |
10 g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | <= 17.0 MPa | <= 2470 psi | ISO/R527 |
| Elongation at Yield | 5.0 % | 5.0 % | ISO/R527 |
| Flexural Modulus | 3.00 GPa <br>@Temperature 23.0 °C |
435 ksi <br>@Temperature 73.4 °F |
ISO 178 |
| Charpy Impact, Notched | 0.300 J/cm² <br>@Temperature 23.0 °C |
1.43 ft-lb/in² <br>@Temperature 73.4 °F |
ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | 87.0 °C <br>@Load 5.001 kg |
189 °F <br>@Load 11.03 lb |
50°C/h; ISO 306 |
| 150 °C <br>@Load 1.00 kg |
302 °F <br>@Load 2.21 lb |
50°C/h; ISO 306 | |
| Glow Wire Test | 750 °C <br>@Thickness 2.00 mm |
1380 °F <br>@Thickness 0.0787 in |
IEC 695-2-1 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
| Mold Temperature | 40.0 - 80.0 °C | 104 - 176 °F | |
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
| Dry Time | 2 - 4 hour | 2 - 4 hour | in circulation dryer |
| 2 - 4 hour | 2 - 4 hour | in desiccant air dryer | |
| Injection Pressure | 40.0 - 110 MPa | 5800 - 16000 psi | |
| Back Pressure | 1.00 - 2.00 MPa | 145 - 290 psi |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Holding Pressure () | 20-40 | % of injection pressure |
| Injection Speed () | High |