| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | 150 °C @Load 1.00 kg |
302 °F @Load 2.21 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYfill PP CIM9040 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
| Vicat Softening Point | 150 °C @Load 1.00 kg |
302 °F @Load 2.21 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYfill PPC B10075 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
| Vicat Softening Point | 150 °C @Load 1.00 kg |
302 °F @Load 2.21 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYfill PPH 30030DNH Polypropylene Homopolymer, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
| Vicat Softening Point | 150 °C @Load 1.00 kg |
302 °F @Load 2.21 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYfill PPH B8065 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
| Vicat Softening Point | 150 °C @Load 1.00 kg |
302 °F @Load 2.21 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYfill PPH B8065 VT1 Polypropylene Homopolymer, Mineral Reinforced, Heat Resistant Information provided by Polykemi AB |
|||
| Vicat Softening Point | 150 °C @Load 1.00 kg |
302 °F @Load 2.21 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYfill PPH B8075 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
| Vicat Softening Point | 150 °C @Load 1.00 kg |
302 °F @Load 2.21 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYfill PPH FR15030 XNH Polypropylene Homopolymer, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
| Vicat Softening Point | 150 °C @Load 1.00 kg |
302 °F @Load 2.21 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYfill PPH T4060 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
| Vicat Softening Point | 150 °C @Load 5.001 kg |
302 °F @Load 11.03 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYform POM C M20 Polyoxymethylene Information provided by Polykemi AB |
|||
| Vicat Softening Point | 150 °C @Thickness 0.250 mm |
302 °F @Thickness 0.00984 in |
ASTM D1525 |
| Mapal Plastics Maplon CFA-HK Polypropylene Sheet Applications: For use with electrical insulation products. For use when flame retardant and static dissipative properties are required. |
|||
| Vicat Softening Point | 150 °C @Load 1.02 kg |
302 °F @Load 2.25 lb |
ISO 306 |
| Borealis Daplen™ EF341AE Polypropylene TPO Compound Daplen™ EF341AE is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q.. |
|||
| Vicat Softening Point | 150 °C @Load 1.02 kg |
302 °F @Load 2.25 lb |
50°C per hour; ISO 306 |
| Total PPH 4054 Polypropylene Homopolymer Polypropylene PPH 4054 is a homopolymer polypropylene with a Melt Flow index of 3 g/10 min.Polypropylene PPH 4054 has been designed for the production of BOPP film with the tenter frame process. Th.. |
|||
| Vicat Softening Point | 150 °C @Load 1.02 kg |
302 °F @Load 2.25 lb |
50°C per hour; ISO 306 |
| Total PPH 4069 Polypropylene Homopolymer, Fiber Polypropylene PPH 4069 is a homopolymer polypropylene with a Melt Flow index of 4 g/10 min.Polypropylene PPH 4069 is intended for extrusion of high tenacity staple fibers for non-woven applications... |
|||
| Vicat Softening Point | 150 °C @Load 0.999 kg |
302 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTACARB 0400 OPALE Polycarbonate Polycarbonate for injection or extrusionOpal, light diffusiveInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 150 °C @Load 0.999 kg |
302 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTACARB 0820 GF Polycarbonate, 10% Glass Filled Polycarbonate with 10% glass fiber reinforcementHigh stiffness, good impact resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 150 °C @Load 0.999 kg |
302 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTACARB 0820 GF V0-5V Flame Retardant Polycarbonate Polycarbonate with 10% glass fiber reinforcementFlame retardant class V0, PBDE free, high stiffness, high dimensional stability, good melt flow, good processability, good light resistanceInformation.. |
|||
| Vicat Softening Point | 150 °C @Load 0.999 kg |
302 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTACARB 0820 GF V0-5V HF Flame Retardant Polycarbonate Polycarbonate with 10% glass fiber reinforcementFlame retardant class V0, antimony, chlorine and bromine free, high stiffness, high dimensional stability, good melt flow rate, good processability, g.. |
|||
| Vicat Softening Point | 150 °C @Load 0.999 kg |
302 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTACARB 1001 Polycarbonate General purpose polycarbonateHigh impact resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 150 °C @Load 0.999 kg |
302 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTACARB 1601 OPALE Polycarbonate Polycarbonate for injection moldingOpal, light diffusiveInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 150 °C @Load 0.999 kg |
302 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTACARB 1601 Polycarbonate General purpose polycarbonateHigh melt flow rate, high impact resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 150 °C @Load 5.10 kg |
302 °F @Load 11.2 lb |
120°C/h; ISO 306 |
| Covestro Makrolon® 3100 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig.. |
|||
| Vicat Softening Point | 150 °C @Load 1.00 kg |
302 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
| Chi Mei Wonderlite® PC-110 Polycarbonate Medium Viscosity |
|||
| Vicat Softening Point | 150 °C @Load 1.00 kg |
302 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
| Chi Mei Wonderlite® PC-122 Polycarbonate High Flow |
|||
| Vicat Softening Point | 150 °C @Load 0.999 kg |
302 °F @Load 2.20 lb |
120°C/min; ASTM D1525/A, ISO 306/A |
| EPICHEM Epilon FR-PC V0 Polycarbonate Characteristics: self-extinguishing V0 at 1,6 mm |
|||
| Vicat Softening Point | 150 °C @Load 5.00 kg |
302 °F @Load 11.0 lb |
120°C/min; ASTM D1525/B, ISO 306/B |
| EPICHEM Epilon G2-PC 10% GF Polycarbonate, 10% Glass Fiber Characteristics: 10% glass fibre filled, good mechanical properties |
|||
| Vicat Softening Point | 150 °C @Load 5.00 kg |
302 °F @Load 11.0 lb |
120°C/min; ASTM D1525/B, ISO 306/B |
| EPICHEM Epilon G4-PC 20% GF Polycarbonate, 20% Glass Fiber Characteristics: 20% glass fibre filled, excellent mechanical properties |
|||
| Vicat Softening Point | 150 °C @Load 5.00 kg |
302 °F @Load 11.0 lb |
120°C/min; ASTM D1525/B, ISO 306/B |
| EPICHEM Epilon PC GF 10 V0 Polycarbonate, 10% Glass Fiber Characteristics: self-extinguishing V0 at 1,6 mm, 10% glass fibre filled |
|||
| Vicat Softening Point | 150 - 155 °C @Load 0.999 kg |
302 - 311 °F @Load 2.20 lb |
120°C/min; ASTM D1525/A, ISO 306/A |
| EPICHEM Epilon PC UVR Polycarbonate, High Impact Characteristics: high fluidity, high impact, UV resistant |
|||
| Vicat Softening Point | 150 °C @Load 1.00 kg |
302 °F @Load 2.21 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYfill PPH T5040 FC Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
| Vicat Softening Point | 150 °C @Load 1.00 kg |
302 °F @Load 2.21 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYfill PPH T5040 FC VT Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||