Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Teijin Films Melinex® 3380 & CORE 1 Polyester Film

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® 3380 & CORE 1 Polyester Film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Melinex® 3380 and Melinex® CORE1 are one-side heat sealable, opaque white polyester films which are ideal in specialty laminated card applications. These films can be heat sealed to themselves and other polyesters, as well as a variety of substrates. The two films are identical except that CORE1 is supplied sheeted with the heat seal surface modified to prevent air entrapment during lamination. CORE1 is required where two layers of CORE1 are laminated to each other as part of the card construction. These two films are currently available at thicknesses of 600 gauge and 1210 gauge.Information provided by DuPont.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ASTM D1505
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 100 %
100 %
ASTM D882A
Film Elongation at Break, TD 80 %
80 %
ASTM D882A
Film Tensile Strength at Break, MD 68.9 MPa
10000 psi
ASTM D882A
Film Tensile Strength at Break, TD 68.9 MPa
10000 psi
ASTM D882A
Heat Seal Strength >= 1800 g/25 mm
>= 3.97 lb/in
DTF (US) Test Method No. 2.49
Thermal Properties Metric English Comments
Shrinkage, MD 2.0 %

@Temperature 190 °C,
Time 300 sec
2.0 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 2.0 %

@Temperature 190 °C,
Time 300 sec
2.0 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Optical Density 0.90

@Thickness 0.152 mm
0.90

@Thickness 0.00600 in
[%]; DTF (US) Test Method 2.30.2
1.8

@Thickness 0.307 mm
1.8

@Thickness 0.0121 in
[%]; DTF (US) Test Method 2.30.2