Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Versaflex™ OM 1040X-1 Thermoplastic Elastomer (TPE)

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer PolyOne Corporation
Trade Name Versaflex™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Versaflex™ OM 1040X-1 Thermoplastic Elastomer (TPE).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
The Versaflex™ OM 1040X-1 is a medical compliant overmolding TPE with very good adhesion to PC or ABS-based plastics. - Good Surface Aesthetics - Rubbery Feel - Soft Touch - Very Good Bond to PC, ABS, PC/ABSColor concentrates with EVA, polypropylene (PP) or LDPE carrier are most suitable for coloring Versaflex™ OM 1040X-1. Typical letdown ratios are 50:1 to 25:1 - loading levels should be as low as possible to minimize the effect on adhesion. A high color match consistency can be obtained by the use of precolored compounds available from GLS. Concentrates based on PVC should not be used. The final determination of color concentrate suitability should be determined by customer trials. trials. Purge thoroughly before and after use of this product with a low flow (0.5 - 2.5 MFR) polyethylene (PE) or polypropylene (PP). Regrind levels up to 20% can be used with Versaflex™ OM 1040X-1 with minimal property loss, provided that the regrind is free of contamination. To minimize losses during molding, the melt temperature should remain as low as possible. The final determination of regrind effectiveness should be determined by the customer. The Versaflex™ OM 1040X-1 has good melt stability. Maximum residence times may vary, depending on the size of the barrel. Generally, the barrel should be emptied if it is idle for periods of 8 - 10 minutes or longer. Drying is not Required Injection Speed: 1 to 5 in/sec 1st Stage - Boost Pressure: 200 to 600 psi 2nd Stage - Hold Pressure: 30% of Boost Hold Time (Thick Part): 4 to 10 sec Hold Time (Thin Part): 1 to 3 secInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 0.918 g/cc
0.918 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.020 - 0.026 cm/cm
0.020 - 0.026 in/in
ASTM D955
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
16 g/10 min

@Load 5.00 kg,
Temperature 200 °C
16 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 42
42
10 sec; ASTM D2240
Tensile Strength at Break 3.47 MPa

@Temperature 23.0 °C
503 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
Tensile Stress 1.24 MPa

@Strain 100 %,
Temperature 23.0 °C
180 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
2.08 MPa

@Strain 300 %,
Temperature 23.0 °C
302 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
Elongation at Break 580 %

@Temperature 23.0 °C
580 %

@Temperature 73.4 °F
Die C2 hr; ASTM D412
Tear Strength 17.5 kN/m
99.9 pli
ASTM D624
Compression Set 22 %

@Temperature 23.0 °C,
Time 79200 sec
22 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395B
Processing Properties Metric English Comments
Rear Barrel Temperature 166 - 188 °C
331 - 370 °F
Middle Barrel Temperature 182 - 199 °C
360 - 390 °F
Front Barrel Temperature 188 - 204 °C
370 - 399 °F
Nozzle Temperature 193 - 216 °C
379 - 421 °F
Melt Temperature 188 - 210 °C
370 - 410 °F
Mold Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Back Pressure 0.000 - 0.862 MPa
0.000 - 125 psi
Screw Speed 75 - 125 rpm
75 - 125 rpm
Descriptive Properties Value Comments
Agency Ratings FDA Unspecified Rating
ISO 10993 Part 4
ISO 10993 Part 5
USP Class VI
Appearance Translucent
Features Good Colorability
Good Moldability
Good Processability
Good Processing Stability
Good Surface Finish
Forms Pellets
Generic Material TPE
Generic Name Thermoplastic Elastomer (TPE)
Manufacturer / Supplier GLS Thermoplastic Elastomers
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant
Suggested Max Regrind 20%
Uses Flexible Grips
Medical/Healthcare Applications
Overmolding
Soft Touch Applications
Transparent or Translucent Parts
Users viewing this material also viewed the following: