| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tear Strength | 17.5 kN/m | 99.9 pli | ASTM D624 |
| PolyOne Versaflex™ OM 1040X-1 Thermoplastic Elastomer (TPE) The Versaflex™ OM 1040X-1 is a medical compliant overmolding TPE with very good adhesion to PC or ABS-based plastics. - Good Surface Aesthetics - Rubbery Feel - Soft Touch - Very Good Bond to PC, A.. |
|||
| Tear Strength | 17.5 kN/m | 99.9 pli | ASTM D624 |
| PolyOne Versaflex™ OM 9-801N Thermoplastic Elastomer (TPE) Versaflex™ OM 9-801N is designed for overmolding onto a wide variety of substrates including PC, ABS, PC/ABS, HIPS, PPO, acetal, acrylic and copolyester. - Bonds to a Variety Of Substrates - Rubber.. |
|||
| Tear Strength | 17.5 kN/m @Temperature 21.0 °C |
99.9 pli @Temperature 69.8 °F |
Die C2 hr; ASTM D624 |
| PolyOne Versalloy™ HC 9210-45N Thermoplastic Elastomer (TPE) Versalloy™ HC 9210-45N is a USP Class VI, TPV alloy targeted for injection molding healthcare applications such as disposable medical items, syringe stoppers, and soft-touch overmolding onto surgic.. |
|||
| Tear Strength | 17.5 kN/m | 99.9 pli | ASTM D624 |
| PolyOne Dynaflex™ G7640-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7640-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
| Tear Strength | 17.5 kN/m | 99.9 pli | ASTM D624 |
| PolyOne Dynaflex™ G7930-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7930-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion.. |
|||
| Tear Strength | 17.5 kN/m @Temperature 23.0 °C, Time 7200 sec |
99.9 pli @Temperature 73.4 °F, Time 2.00 hour |
ASTM D624 |
| PolyOne Dynaflex™ G7930-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7930-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. - NSF 51 approved - FDA (see Notes) - Overmold Adhesion to Polypropylene - Soft To.. |
|||
| Tear Strength | 17.5 kN/m @Temperature 23.0 °C, Time 7200 sec |
99.9 pli @Temperature 73.4 °F, Time 2.00 hour |
ASTM D624 |
| PolyOne Dynaflex™ G7930-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7930-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion.. |
|||
| Tear Strength | 17.5 kN/m | 99.9 pli | ASTM D624 |
| PolyOne Dynaflex™ G7940-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7940-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
| Tear Strength | 17.5 kN/m | 99.9 pli | ASTM D624 |
| PolyOne Dynaflex™ G7940-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7940-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion.. |
|||
| Tear Strength | 17.5 kN/m | 99.9 pli | ASTM D624 |
| PolyOne Dynaflex™ G7940-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7940-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
| Tear Strength | 17.5 kN/m | 99.9 pli | ASTM D624 |
| PolyOne Dynaflex™ G7940-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7940-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion.. |
|||
| Tear Strength | 17.5 kN/m | 99.9 pli | ASTM D624 |
| PolyOne Dynaflex™ G7640-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7640-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhe.. |
|||
| Tear Strength | 17.5 kN/m | 99.9 pli | ASTM D624 |
| PolyOne Dynaflex™ G7930-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7930-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. - NSF 51 approved - FDA (see Notes) - Overmold Adhesion to Polypropylene - Soft To.. |
|||
| Tear Strength | 17.5 kN/m | 99.9 pli | ASTM D624 |
| PolyOne Dynalloy™ OBC 8100-N50 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8100-N50 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring t.. |
|||
| Tear Strength | 17.5 - 105 kN/m | 99.9 - 599 pli | Average value: 53.8 kN/m Grade Count:29 |
| Overview of materials for PVC, Extruded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
| Tear Strength | 17.5 kN/m | 99.9 pli | ASTM D624 |
| Multibase Multi-Flex® TPE 6568 C 1 NATURAL This product was designed for 2 shot airbag covers with lower tensile strength than currently in use. The moisture content is 1%. The fogging test value is 70% according to ASTM GM 9305P. Multi-F.. |
|||
| Tear Strength | 17.5 kN/m | 99.9 pli | ASTM D624 |
| Multibase Multi-Flex® TPE A 5402 BLK The burn rate is 0.7 in/min based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
| Tear Strength | 17.5 kN/m | 99.9 pli | ASTM D1004-94 |
| Saint-Gobain Fluran® F-5500-A Fluoroelastomer Tubing Fluran® Severe Environment Tubing has the physical and chemical characteristics that make it ideal for severe environments, such as dry cleaning fluid lines and solvent recovery systems, where othe.. |
|||
| Tear Strength | 17.5 kN/m | 99.9 pli | Die C, 510 mm/min; ASTM D624 |
| PolyOne Elastamax™ XL-0153-24 Styrene Butadiene Block Copolymer (SBC)
(discontinued **) A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in acco.. |
|||