Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 16 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 16 g/10 min

@Load 5.00 kg,
Temperature 200 °C
16 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
PolyOne Versaflex™ OM 1040X-1 Thermoplastic Elastomer (TPE)
The Versaflex™ OM 1040X-1 is a medical compliant overmolding TPE with very good adhesion to PC or ABS-based plastics. - Good Surface Aesthetics - Rubbery Feel - Soft Touch - Very Good Bond to PC, A..
Melt Flow 16 g/10 min

@Load 10.0 kg,
Temperature 220 °C
16 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
SABIC Innovative Plastics Cycolac® INP562 ABS
SABIC INP562 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..
Melt Flow 16 g/10 min

@Load 10.0 kg,
Temperature 220 °C
16 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
SABIC Innovative Plastics Cycolac® INP562 ABS+SAN
SABIC INP562 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..
Melt Flow 16 g/10 min

@Load 10.0 kg,
Temperature 220 °C
16 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
SABIC Innovative Plastics Cycolac® INP572 ABS
High molecular weight SAN, functions as a carrier resin for color concentrates. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to pro..
Melt Flow 16 g/10 min

@Load 10.0 kg,
Temperature 220 °C
16 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
SABIC Innovative Plastics Cycolac® MG37CR ABS
High performance, injection molding ABS. Overall balance of physical properties, good processability and chemical resistance.This data was supplied by SABIC-IP for the Americas region.
Melt Flow 16 g/10 min

@Load 5.00 kg,
Temperature 220 °C
16 g/10 min

@Load 11.0 lb,
Temperature 428 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Cycolac® S157 ABS (Europe-Africa-Middle East)
CYCOLAC S157 is a high flow flame retardant ABS with good processability developed for applications requiring UL94 V0 at reduced wall thickness.This data was supplied by SABIC-IP for the Europe-Afri..
Melt Flow 16 g/10 min

@Load 5.00 kg,
Temperature 220 °C
16 g/10 min

@Load 11.0 lb,
Temperature 428 °F
ISO 1133
SABIC Innovative Plastics Cycolac® S701S ABS (Europe-Africa-Middle East)
CYCOLAC S701S is a new developed ABS providing a superior balance of properties. Its wide processing window, excellent flow and good mechanical properties give this material an excellent fit in appl..
Melt Flow 16 g/10 min

@Load 10.0 kg,
Temperature 220 °C
16 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
SABIC Innovative Plastics Cycolac® S702S ABS (Europe-Africa-Middle East)
CYCOLAC S702S is a high impact ABS combined with a good flow. This material is developed for enclosures and housings found in appliances and automotive industries. Cycolac S702S is anti-dust equiped..
Melt Flow 16 g/10 min

@Load 5.00 kg,
Temperature 230 °C
16 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
Premix Thermoplastics PRE-ELEC® PP 1395
PRE-ELEC PP 1395 is a dissipative thermoplastic compound based on polypropylene. The electrical dissipation is achieved by using special conductive carbon black. In addition to stable surface resist..
Melt Flow 16 g/10 min

@Load 5.00 kg,
Temperature 260 °C
16 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D 1238
SABIC Innovative Plastics Cycoloy® CP8930 PC+ABS (Europe-Africa-Middle East)
High heat, PC/ABS for automotive electro plating applications, excellent balance in flow/impactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Melt Flow 16 g/10 min

@Load 2.16 kg,
Temperature 260 °C
16 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D 1238
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc..
Melt Flow 16 g/10 min

@Load 2.16 kg,
Temperature 250 °C
16 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS (Europe-Africa-Middle East)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la..
Melt Flow 16 - 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
16 - 20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 2060V (60118) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 16 g/10 min

@Load 2.16 kg,
Temperature 260 °C
16 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
PTS PCA-2201NH Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Melt Flow 16 g/10 min

@Load 1.20 kg,
Temperature 300 °C
16 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® SLX1231D PC Copolymer (Asia Pacific)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region.
Melt Flow 16 g/10 min

@Load 1.20 kg,
Temperature 300 °C
16 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® XHT1143 PC (Asia Pacific)
XHT1143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is the lowest heat, UV stabilized product in the LEXAN* XHT portfolio. It is available in a range of opaque and limited ..
Melt Flow 16 g/10 min

@Load 1.20 kg,
Temperature 300 °C
16 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® DMX1214 PC Copolymer
Lexan* DMX1214 resin is an improved flow, transparent copolycarbonate resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region.
Melt Flow 16 g/10 min

@Load 1.20 kg,
Temperature 300 °C
16 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® SLX1231T PC Copolymer
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas region.
Melt Flow 16 - 56 g/10 min

@Load 21.6 kg,
Temperature 190 °C
16 - 56 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Kazanorgsintez PE2NT26-13 High Density Polyethylene Composite
Production Method: Copolymerization of eythylene at low pressure in presence of complex catalysts using gaseous-phase method. Application: Composition is intended for injection molding processin..
Melt Flow 16 g/10 min

@Load 3.80 kg,
Temperature 230 °C
16 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238 (I)
LG Chemical HIPS MI770 PS, Impact Modified
Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica..
Melt Flow 16 g/10 min

@Load 6.60 kg,
Temperature 337 °C
16 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D 1238
SABIC Innovative Plastics Ultem 1110R PEI
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region.
Melt Flow 16 g/10 min

@Load 6.60 kg,
Temperature 337 °C
16 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D 1238
SABIC Innovative Plastics Ultem 1110V PEI
Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Americas region.
Melt Flow 16 g/10 min

@Load 6.60 kg,
Temperature 337 °C
16 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D 1238
SABIC Innovative Plastics Ultem 1110V PEI (Europe-Africa-Middle East)
Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Melt Flow 16 g/10 min

@Load 5.00 kg,
Temperature 220 °C
16 g/10 min

@Load 11.0 lb,
Temperature 428 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Ultem HATX200 PEI+PCE
High flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compli..
Melt Flow 16 g/10 min

@Load 5.00 kg,
Temperature 220 °C
16 g/10 min

@Load 11.0 lb,
Temperature 428 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Ultem HATX200 PEI+PCE (Asia Pacific)
High flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compli..
Melt Flow 16 g/10 min

@Load 5.00 kg,
Temperature 220 °C
16 g/10 min

@Load 11.0 lb,
Temperature 428 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Ultem HATX200 PEI+PCE (Europe-Africa-Middle East)
High flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compli..
Melt Flow 16 - 26 g/10 min

@Load 3.80 kg,
Temperature 230 °C
16 - 26 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Solvay Specialty Polymers Solef® 9007 Polyvinylidene Fluoride (PVDF)
Solef® 9007 PVDF homopolymer has low viscosity and is used in film extrusion and injection molding.Features: Homopolymer; Low ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 53...
Melt Flow 16 g/10 min

@Load 5.00 kg,
Temperature 250 °C
16 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics Xenoy® 1105 PBT+PC (Asia Pacific)
PBT/PC blend, injection molding grade, non-reinforced, impact modified, excellent toughness at low temperatures, very good paintability
Melt Flow 16 g/10 min

@Load 5.00 kg,
Temperature 200 °C
16 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Styrolution Styrolux 656C SBC
Styrolux 656C is a high flow thermoplastic injection molding styrene-butadiene block copolymer. It has crystal clarity, good toughness, good stiffness, and warpage resistance for general molding ap..
Melt Flow 16 g/10 min

@Load 5.00 kg,
Temperature 260 °C
16 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
Techmer ES Plastiblend® APC100 UV
Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV ResistanceInformation provided by TP Composites, Inc.
Copyright © lookpolymers.com All Rights Reserved