| Category | Polymer , Thermoplastic , Nylon , Nylon 6 |
| Manufacturer | PolyOne Corporation |
| Trade Name | Gravi-Tech™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Gravi-Tech™ GRV-NY-060-CU Polyamide 6 (Nylon 6).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 5.99 g/cc | 5.99 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm | 0.0030 - 0.0050 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 45.5 MPa | 6600 psi | Type I, 5.1 mm/min; ASTM D638 |
| Elongation at Break | 1.2 % | 1.2 % | Type I, 5.1 mm/min; ASTM D638 |
| Tensile Modulus | 16.5 GPa | 2390 ksi | Type I, 5.1 mm/min; ASTM D638 |
| Flexural Yield Strength | >= 70.0 MPa | >= 10200 psi | ASTM D790 |
| Flexural Modulus | 14.5 GPa | 2100 ksi | ASTM D790 |
| Charpy Impact Unnotched | >= 0.600 J/cm² @Temperature 23.0 °C |
>= 2.86 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| Charpy Impact, Notched | >= 0.250 J/cm² @Temperature 23.0 °C |
>= 1.19 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 152 °C @Thickness 6.35 mm |
306 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 260 - 288 °C | 500 - 550 °F | |
| Mold Temperature | 82.2 - 149 °C | 180 - 300 °F | |
| Drying Temperature | 79.4 °C | 175 °F | |
| Dry Time | 4.00 hour | 4.00 hour |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Features | Non-Toxic | |
| Forms | Pellets | |
| Generic Material | Nylon 6 | |
| Generic Name | Polyamide 6 (Nylon 6) | |
| Processing Method | Injection Molding | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Industrial Applications | |
| Medical/Healthcare Applications | ||
| Projectiles | ||
| Sporting Goods | ||
| Weighting & Balancing |