Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyplastics Tepcon M450 Acetal-copolymer (POM), Super High Fluidity, High Cycle

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced
Manufacturer Polyplastics Co.
Trade Name Tepcon
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyplastics Tepcon M450 Acetal-copolymer (POM), Super High Fluidity, High Cycle.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by PolyPlastics.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 63.0 MPa
9140 psi
ISO 527-1, 2
Elongation at Break 27 %
27 %
ISO 527-1, 2
Tensile Modulus 2.80 GPa
406 ksi
ISO 527-1, 2
Flexural Strength 89.0 MPa
12900 psi
ISO 178
Flexural Modulus 2.55 GPa
370 ksi
ISO 178
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 110 µm/m-°C

@Temperature 20.0 °C
61.1 µin/in-°F

@Temperature 68.0 °F
ISO 11359-2
CTE, linear, Transverse to Flow 110 µm/m-°C

@Temperature 20.0 °C
61.1 µin/in-°F

@Temperature 68.0 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
ISO 75-1, 2
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
IEC 60093
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
IEC 60093
Dielectric Strength 19.0 kV/mm
483 kV/in
IEC 60243-1
Comparative Tracking Index >= 600 V
>= 600 V
IEC 60112