| Category | Polymer , Thermoplastic , Nylon , Nylon 66 |
| Manufacturer | PolyOne Corporation |
| Trade Name | Bergamid™ |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | PolyOne Bergamid™ A700 G25 HW UF Polyamide 66 (Nylon 66).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.40 g/cc | 0.0506 lb/in³ | ±0.03 g/cm³; DIN 53479 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 130 MPa @Temperature 23.0 °C |
18900 psi @Temperature 73.4 °F |
ISO 527-2/5 |
| Elongation at Break | 2.5 % @Temperature 23.0 °C |
2.5 % @Temperature 73.4 °F |
ISO 527-2/5 |
| Tensile Modulus | 10.0 GPa @Temperature 23.0 °C |
1450 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
| Charpy Impact Unnotched | 5.50 J/cm² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
| Charpy Impact, Notched | 0.700 J/cm² @Temperature 23.0 °C |
3.33 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 261 °C | 502 °F | ISO 3146 |
| Deflection Temperature at 0.46 MPa (66 psi) | 250 °C | 482 °F | Unannealed; ISO 75-2/B |
| Deflection Temperature at 1.8 MPa (264 psi) | 240 °C | 464 °F | Unannealed; ISO 75-2/A |
| Flammability, UL94 | V-0 @Thickness 0.800 mm |
V-0 @Thickness 0.0315 in |
ALL; Internal Method |
| Glow Wire Test | 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
0.8 mm wire; Ignition Temperature; IEC 60695-2-13 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | Heat Stabilizer | |
| Features | Flame Retardant | |
| Halogen Free | ||
| Heat Stabilized | ||
| Low (to None) Phosphorus Content | ||
| Filler / Reinforcement | Glass Fiber Reinforcement, 25% Filler by Weight | |
| Forms | Pellets | |
| Generic Material | Nylon 66 | |
| Generic Name | Polyamide 66 (Nylon 66) | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| RoHS Compliance | RoHS Compliant |