| Category | Polymer , Thermoplastic , Nylon , Nylon 66 |
| Manufacturer | PolyOne Corporation |
| Trade Name | Bergamid™ |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | PolyOne Bergamid™ A70 UF natur V0 Polyamide 66 (Nylon 66).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.14 g/cc @Temperature 23.0 °C |
0.0412 lb/in³ @Temperature 73.4 °F |
±0.03 g/cm³; DIN 53479 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 70.0 MPa @Temperature 23.0 °C |
10200 psi @Temperature 73.4 °F |
ISO 527-2/50 |
| Elongation at Yield | 4.0 % @Temperature 23.0 °C |
4.0 % @Temperature 73.4 °F |
ISO 527-2/50 |
| Tensile Modulus | 3.50 GPa @Temperature 23.0 °C |
508 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
| Charpy Impact Unnotched | NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
ISO 179/1eU |
| Charpy Impact, Notched | 0.500 J/cm² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 260 °C | 500 °F | ISO 3146 |
| Flammability, UL94 | V-0 @Thickness 0.400 - 3.00 mm |
V-0 @Thickness 0.0157 - 0.118 in |
UL 94 |
| Glow Wire Test | 960 °C @Thickness 0.400 - 3.00 mm |
1760 °F @Thickness 0.0157 - 0.118 in |
Flammability Index; IEC 60695-2-12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
| Comparative Tracking Index | 600 V | 600 V | Solution A; IEC 60112 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Opaque | |
| Forms | Pellets | |
| Generic Material | Nylon 66 | |
| Generic Name | Polyamide 66 (Nylon 66) | |
| K-Value | 74.0 to 78.0 | No Standard; 96% H2SO4 |
| Regional Availability | Europe | |
| RoHS Compliance | RoHS Compliant |