| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.14 g/cc | 1.14 g/cc | ISO 1183 |
| Water Absorption | 8.0 % | 8.0 % | ISO 62 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 55.0 MPa | 7980 psi | ISO 527 |
| Elongation at Yield | >= 100 % | >= 100 % | ISO 527 |
| Modulus of Elasticity | 1.65 GPa | 239 ksi | ISO 527 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+12 ohm-cm | >= 1.00e+12 ohm-cm | VDE 0303 |
| Surface Resistivity per Square | >= 1.00e+12 ohm | >= 1.00e+12 ohm | VDE 0303 |
| Dielectric Constant | 3.8 @Frequency 1.00e+6 Hz |
3.8 @Frequency 1.00e+6 Hz |
DIN 53483 |
| Dielectric Strength | 18.0 kV/mm | 457 kV/in | VDE 0303 |
| Dielectric Loss Index | 0.060 @Frequency 1.00e+6 Hz |
0.060 @Frequency 1.00e+6 Hz |
DIN 53483 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Aromatic Resistance | limited | |
| Color | Natural | |
| Hydrocarbonate Resistance | limited | |
| Ketone Resistance | limited | |
| Resistance Against Hot Water | limited |