| Category | Polymer , Thermoplastic , Polyethylene (PE) , HDPE |
| Manufacturer | Plastcom spol. s r.o. |
| Trade Name | PLASTALEN® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Plastcom PLASTALEN® EH 91 N Polyethylene.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.950 g/cc | 0.0343 lb/in³ | STN EN ISO 1183-1 |
| Melt Flow | 4.0 - 8.0 g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C |
4.0 - 8.0 g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F |
STN EN ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 30.0 MPa | 4350 psi | STN EN ISO 527-2 |
| Elongation at Break | 150 % | 150 % | STN EN ISO 527-2 |
| Tensile Modulus | 1.50 GPa | 218 ksi | STN EN ISO 527-2 |
| Flexural Strength | 40.0 MPa | 5800 psi | STN EN ISO 178 |
| Flexural Modulus | 1.10 GPa | 160 ksi | STN EN ISO 178 |
| Charpy Impact Unnotched | NB <br>@Temperature 23.0 °C |
NB <br>@Temperature 73.4 °F |
STN EN ISO 179 |
| Charpy Impact, Notched | 0.500 J/cm² <br>@Temperature 23.0 °C |
2.38 ft-lb/in² <br>@Temperature 73.4 °F |
STN EN ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 145 °C | 293 °F | STN EN 11357-1 |
| Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | STN EN ISO 75-2 (A) |
| Vicat Softening Point | 150 °C | 302 °F | STN EN ISO 306 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
| Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
| Drying Temperature | 80.0 °C <br>@Time 14400 sec |
176 °F <br>@Time 4.00 hour |
|
| Moisture Content | 0.20 % | 0.20 % | STN EN ISO 3344 |
| Injection Pressure | 60.0 - 70.0 MPa | 8700 - 10200 psi |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Blue |