Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Permabond MM115P Pure Anaerobic Threadlocker

Category Polymer , Adhesive , Thermoset
Manufacturer Permabond
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Permabond MM115P Pure Anaerobic Threadlocker.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Permabond® MM115 PURE Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking metal bolts, nuts and screws that may require disassembly for service and maintenance. Its medium strength allows disassembly with ordinary tools. Cure is fast and reliable on steel, cadmium, zinc and other plated fasteners. Permabond MM115 PURE has been designed for use in contact with potable water. Features & Benefits: NSF/ANSI 61 Certified drinking water system component Controlled off-torque Full cure at room temperature Lubricates threads for easier assembly Provides corrosion protections Non-drip thixotropic Environmentally friendly – 100% solids Information provided by Permabond.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Uncured
Viscosity 1300 cP

@Temperature 25.0 °C
1300 cP

@Temperature 77.0 °F
at 20 rpm vibration
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Mechanical Properties Metric English Comments
Adhesive Bond Strength 10.0 MPa
1450 psi
steel collar and pin shear; ISO 10123
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 149 °C
300 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 11.0 kV/mm
279 kV/in
Processing Properties Metric English Comments
Cure Time 4.98 min

@Temperature 23.0 °C
0.0830 hour

@Temperature 73.4 °F
Brass, handling strength
10.2 min

@Temperature 23.0 °C
0.170 hour

@Temperature 73.4 °F
M10 steel, handling strength
15.0 min

@Temperature 23.0 °C
0.250 hour

@Temperature 73.4 °F
Zinc, handling strength
30.0 min

@Temperature 23.0 °C
0.500 hour

@Temperature 73.4 °F
Brass, working strength
30.0 min

@Temperature 23.0 °C
0.500 hour

@Temperature 73.4 °F
M10 steel, working strength
60.0 min

@Temperature 23.0 °C
1.00 hour

@Temperature 73.4 °F
Zinc, working strength
360 min

@Temperature 23.0 °C
6.00 hour

@Temperature 73.4 °F
Zinc, full strength
360 min

@Temperature 23.0 °C
6.00 hour

@Temperature 73.4 °F
M10 steel, full strength
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Colorless to Light Amber
Uncured
Maximum Gap Fill (mm) 0.15
Strength Retention 20% at 150°C
Relative to 0°C
70% at 100°C
Relative to 0°C
90% at 50°C
Relative to 0°C
Torque Strength (N m) 16
M10 steel, break
7
M10 steel, prevail
UV Fluorescence No