Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
ASTM D 696 |
Polimeri Europa Sinkral® C 442 ABS Resin Sinkral C 442 is a heat resistant injection molding grade offering good flow and impact resistance together with excellent thermal stability during processing. Designation: Thermoplastic ISO 2580-AB.. |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | ASTM D696 |
Polimeri Europa Sinkral® PD L 322 ABS Resin Sinkral PD L 322 by continuous mass, is a general purpose, high flow injection molding grade having good impact resistance coupled with an excellent gloss.Applications: Widely used in the small and.. |
|||
CTE, linear | 90.0 µm/m-°C @Temperature 23.0 - 100 °C |
50.0 µin/in-°F @Temperature 73.4 - 212 °F |
|
Quadrant EPP Nylatron® MC901 PA 6, blue, cast (ISO Data) This modified cast nylon 6 grade with its distinctive blue colour exhibits higher toughness, flexibility and fatigue resistance than Ertalon 6 PLA. It has proved to be an excellent material for gear.. |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | |
Permabond 105 Cyanoacrylate, for difficult rubbers PERMABOND® 105 is a low viscosity high purity cyanoacrylate adhesive. It is ideal for use on hard-to-bond plastics and rubbers such as natural rubber, EPDM and butyl rubber. Cyanoacrylate adhesives.. |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | |
Permabond LM012 Anaerobic Threadsealant Permabond® LM012 is an unfilled, medium viscosity anaerobic adhesive. Its major benefit as related to other pipe sealants is that it is an unfilled resin that is compatible with hydraulic fluids. I.. |
|||
CTE, linear | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
ASTM D 696 |
Polimeri Europa Edistir RK Polystyrene
(discontinued **) UL94 V-0, flame retarded, high impact polystyrene. This grade is suitable for injection moulding. It combines high mechanical strength, heat resistance and good processability.
Designation: Thermopl.. |
|||
CTE, linear | 90.0 - 140 µm/m-°C @Temperature 30.0 - 300 °C |
50.0 - 77.8 µin/in-°F @Temperature 86.0 - 572 °F |
Average value: 113 µm/m-°C Grade Count:2 |
Overview of materials for Polytetrafluoroethylene (PTFE), Conductive Carbon Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Conductive Carbon Filled". Each property range of values reported is min.. |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 80/TF/18/SI/2 Polyacetal-copolymer, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 80-0837-1 Polyacetal-copolymer, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | ASTM D696 |
Gromax CCP PBT 1100-220S Product Description: PBT unreinforced and impact-modified injection molding grade. Characteristics:Low warp age, high toughness and excellent dimensional stabilityExcellent glossy surface and less-g.. |
|||
CTE, linear | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
DIN 53752; ASTM D696 |
Kolon KOPA® KN132VO Flame Retardant Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
CTE, linear | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Panel Pro ABS UV-Resistant Embossed Sheet Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
CTE, linear | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech SolarKote® /ABS Weatherable Sheet Description: Weatherable SheetSolarKote is a registered trademark of Atofina Chemicals, Inc..Information provided by Spartech. |
|||
CTE, linear | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech SparAlloy Rigid Foamed ABS Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | ASTM D696 |
Samyang Tribit® 1700 PBT, Middle Viscosity Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1700 is a middle viscosity grade.Informatio.. |
|||
CTE, linear | 90.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 53752 |
CP-Polymer-Technik Wellamid® 6000/50 HWUVCP Nylon 6, Impact Modified Until 0°C, UV Stabilized, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | ASTM D696 |
Americas Styrenics EB6755 High Impact Polystyrene Product CharacteristicsGood Environmental Stress Crack Resistance (ESCR)Good practical toughnessDeep draw thermoforming capableGood low temperature impactFood Contact CompliantTypical ApplicationsPa.. |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | ASTM D696 |
Americas Styrenics STYRON A-TECH® 1170 High Impact Polystyrene Product CharacteristicsGood impact resistanceConsistent colorabilityEasy processingFood Contact CompliantUL Classification 94HBTypical ApplicationsExtruded SheetSmall AppliancesRefrigeration Accesso.. |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | ASTM D696 |
Americas Styrenics STYRON® 421 High Impact Polystyrene Product CharacteristicsStiffness/FlowHeat resistanceContact clarityFood Contact CompliantUL Classification 94HBTypical ApplicationsAppliancesRefrigerationPackaging/disposablesConsumer electronicsInf.. |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | ASTM D696 |
Americas Styrenics STYRON® 678D High Heat Crystal Polystyrene Product CharacteristicsHigh heat resistanceExcellent clarityGood moldabilityFood Contact CompliantTypical ApplicationsDisposable cutleryHousewaresCompact disc and DVD jewel boxesDesk organizersInfor.. |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | ASTM D696 |
Americas Styrenics STYRON® 686E High Heat Crystal Polystyrene Product CharacteristicsExceptional balance between heat resistance, toughness and flowGood dimensional stability and excellent clarityFood Contact CompliantTypical ApplicationsFoamed PS sheets used .. |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | ASTM D696 |
Americas Styrenics STYRON® 487 High Impact Polystyrene Product CharacteristicsGood TrimmabilityToughnessHeat resistanceFood Contact CompliantUL Classification 94HBTypical ApplicationsLidsAppliancesPackaging/disposablesHousewaresInformation provided by A.. |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | ASTM D696 |
Americas Styrenics STYRON® 665 High Heat Crystal Polystyrene Product CharacteristicsAdditive freeFood Contact CompliantTypical ApplicationsFilmInformation provided by AmericasStyrenics LLC. |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | |
Permabond 792 Cyanoacrylate, Surface insensitive PERMABOND® 792 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar.. |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | ASTM D696 |
Gromax PBT 1200-211D Product Description: PBT unreinforced middle viscosity injection molding grade.Characteristics:Excellent electrical propertyExcellent temperature resistance, high heat distortion temperature.Excelle.. |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | |
Permabond A1046 Anaerobic Retainer Permabond® A1046 is a rapid curing adhesive designed to provide permanent locking and sealing of metal parts such as bearings, gears, pulleys and threaded components. It exhibits high strength and .. |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | |
Permabond A134 Anaerobic Retainer Permabond® A134 is a high-strength anaerobic product designed for the permanent locking and sealing of metal parts. Its 'non-drip' formulation makes it suitable for use on larger fittings, coarse t.. |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | ASTM D696 |
Gromax PBT 1200-211M Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | ASTM D696 |
Samyang Tribit® 1800 PBT, High Viscosity Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1800 is a high viscosity grade.Information .. |