| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Flow |
40
g/10 min <br>@Load 3.80 kg,<br> Temperature 230 °C
|
40
g/10 min <br>@Load 8.38 lb,<br> Temperature 446 °F
|
ASTM D-1238 |
|
Plaskolite Optix® CA - 42 General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
|
|||
| Melt Flow |
40
g/10 min <br>@Load 0.325 kg,<br> Temperature 270 °C
|
40
g/10 min <br>@Load 0.716 lb,<br> Temperature 518 °F
|
|
|
Plastcom SLOVASTER® B1 BT PBT, basic type
FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of..
|
|||
| Melt Flow |
40
g/10 min <br>@Load 3.80 kg,<br> Temperature 230 °C
|
40
g/10 min <br>@Load 8.38 lb,<br> Temperature 446 °F
|
ASTM D-1238 |
|
Plaskolite West Optix® CA - 42 General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
|
|||
| Melt Flow |
40
g/10 min <br>@Load 5.00 kg,<br> Temperature 190 °C
|
40
g/10 min <br>@Load 11.0 lb,<br> Temperature 374 °F
|
|
|
Total Finaprene® 602 Styrene-Butadiene TPE Copolymer Compound, Formulated to 58 Shore A
(discontinued **)
Styrene-Butadiene CopolymerDescription: Finaprene® 602 is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its broad molecular weight distribution, Finaprene® 60..
|
|||
| Melt Flow |
40
g/10 min <br>@Load 2.16 kg,<br> Temperature 190 °C
|
40
g/10 min <br>@Load 4.76 lb,<br> Temperature 374 °F
|
ASTM D 1238 |
|
Chevron Phillips KN 230 LDPE Injection Molding Resin
(discontinued **)
Resin Type: Homopolymer; ASTM D 4976 Classification: PE 111, A 22200Characteristics: Good Flexibility, Excellent Flow, Good Warping Resistance, Good Mold Release, Moderate ESCRApplications:Houseware..
|
|||
| Melt Flow |
40
g/10 min <br>@Load 2.16 kg,<br> Temperature 190 °C
|
40
g/10 min <br>@Load 4.76 lb,<br> Temperature 374 °F
|
ASTM D 1238 |
|
Chevron Phillips KN 230B LDPE Injection Molding Resin
(discontinued **)
Resin Type: Homopolymer; Mold Release Agent Added; ASTM D 4976 Classification: PE 111, A 22200Characteristics: Good Flexibility, Excellent Flow, Good Warping Resistance, Good Mold Release, Moderate ..
|
|||
| Melt Flow |
40
g/10 min <br>@Load 10.0 kg,<br> Temperature 220 °C
|
40
g/10 min <br>@Load 22.0 lb,<br> Temperature 428 °F
|
ASTM D1238 |
|
Ineos ABS Lustran® 228 Specialty, High Productivity
(discontinued **)
Information provided by Bayer Corporation, Plastics DivisionLANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with La..
|
|||
| Melt Flow |
40
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
40
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer (Europe-Africa-Middle East)
40 MFR LEXAN High Flow Ductile Copolymer
|
|||
| Melt Flow |
40
g/10 min <br>@Load 10.0 kg,<br> Temperature 220 °C
|
40
g/10 min <br>@Load 22.0 lb,<br> Temperature 428 °F
|
ASTM D1238 |
|
LG Chemical HF380I ABS, High Flow
Feature: Injection Molding, High Flow, Good PaintabilityApplication: Painting Products of Motor Cycle)CAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Melt Flow |
40
g/10 min <br>@Load 10.0 kg,<br> Temperature 220 °C
|
40
g/10 min <br>@Load 22.0 lb,<br> Temperature 428 °F
|
ASTM D1238 |
|
LG Chemical HF380XC ABS, High Flow, High Surface Gloss
Feature: Injection Molding, High Flow, High Surface GlossApplication: High melt flow index is suitable for injection molding of large and complicated part. High thermal stabilities enables to expres..
|
|||
| Melt Flow |
40
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
40
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ASTM D1238 |
|
Ineos L40N-00 Polypropylene Impact Copolymer
L40N-00 is a nucleated high flow polypropylene, medium impact copolymer for injection molding applications. This resin exhibits an excellent balance of resin flow and mechanical properties. This res..
|
|||
| Melt Flow |
40
-
60
g/10 min <br>@Load 10.0 kg,<br> Temperature 190 °C
|
40
-
60
g/10 min <br>@Load 22.0 lb,<br> Temperature 374 °F
|
ISO 1133 |
|
Lubrizol Advanced Materials Pearlbond® 12F75UV Thermoplastic Polyurethane
Pearlbondâ„¢ 12F75UV is a UV-resistant standard polyester-based TPU supplied in form of translucent, colorless pellets, featuring a low melting point and very low gel content. Processed by extrus..
|
|||
| Melt Flow |
40
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
40
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ASTM D1238 |
|
Multibase Multi-Flex® A 1540 Natural TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodSoftUV Resistance, Go..
|
|||
| Melt Flow |
40
g/10 min <br>@Load 5.00 kg,<br> Temperature 266 °C
|
40
g/10 min <br>@Load 11.0 lb,<br> Temperature 511 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics Valox® 4022 PBT (Europe-Africa-Middle East)
VALOX 4022 is a 20% high strength glass fibre reinforced PBT injection moulding resin, with improved mechanical properties. Applications : Spotlights, appliance housings and handles.
|
|||
| Melt Flow |
40
g/10 min <br>@Load 5.00 kg,<br> Temperature 266 °C
|
40
g/10 min <br>@Load 11.0 lb,<br> Temperature 511 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics Valox® 553 PBT (Europe-Africa-Middle East)
VALOX 553 is a 30% glass fibre reinforced, flame retardant PBT+PC blend with good warpage characteristics. Applications: appliance handles, spotlights, electric motors, pumphousings.
|
|||
| Melt Flow |
40
g/10 min <br>@Load 2.16 kg,<br> Temperature 265 °C
|
40
g/10 min <br>@Load 4.76 lb,<br> Temperature 509 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics Valox® EH7025AG PBT+PET
Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application.
|
|||
| Melt Flow |
40
g/10 min <br>@Load 10.0 kg,<br> Temperature 220 °C
|
40
g/10 min <br>@Load 22.0 lb,<br> Temperature 428 °F
|
from MVR; ISO 1033 |
|
Sax Polymers SAXLAC 340Q Acrylonitrile Butadiene Styrene
Saxalac 340Q is an siliconized, UV protected, high impact resistant and easy flowing ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tes..
|
|||
| Melt Flow |
40
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
40
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ASTM D1238 |
|
SCG Chemicals EL-Proâ„¢ P841J Polypropylene Injection Molding
Key Characteristics:Excellent flowabilityExcellent processabilityHigh stiffnessSuitable for complex parts and large partsContains UV stabilizer and anti-static agentRecommended Applications:Electric..
|
|||
| Melt Flow |
40
g/10 min <br>@Load 5.00 kg,<br> Temperature 224 °C
|
40
g/10 min <br>@Load 11.0 lb,<br> Temperature 435 °F
|
ASTM D1238 |
|
Lubrizol Pellethane® 2363-65D Thermoplastic Polyurethane Elastomer
Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
|
|||
| Melt Flow |
40
g/10 min <br>@Load 2.16 kg,<br> Temperature 190 °C
|
40
g/10 min <br>@Load 4.76 lb,<br> Temperature 374 °F
|
ASTM D1238 |
|
Westlake EM184AA Low Density Polyethylene
WESTLAKE low-density polyethylene EM184 is a low density injection-molding formulation suggested for the production of closures where a high melt index is needed to meet shrinkage requirements and f..
|
|||
| Melt Flow |
40
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
40
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ISO 1133 |
|
Total PPR 10232 Random Copolymer Polypropylene, Injection Molding
Total Petrochemicals PPR 10232 is a nucleated and antistatic random copolymer polypropylene with a melt flow index of 40 g/10min for the injection molding of articles with high transparency and exce..
|
|||
| Melt Flow |
40
g/10 min <br>@Load 2.16 kg,<br> Temperature 190 °C
|
40
g/10 min <br>@Load 4.76 lb,<br> Temperature 374 °F
|
ASTM D1238 |
|
ExxonMobil LDPE LD 637.LI Low Density Polyethylene Resin
Product Description: LD 637.LI is a high melt index LDPE homopolymer intended for injection molding or compounding applications requiring high flow. It is ideal for tamper-evident, tear-to-open clos..
|
|||
| Melt Flow |
40
g/10 min <br>@Load 5.00 kg,<br> Temperature 275 °C
|
40
g/10 min <br>@Load 11.0 lb,<br> Temperature 527 °F
|
ISO 1133 |
|
BASF Ultramid® A34 01 PA66 (Conditioned)
Ultramid A34 01 is an intermediate visosity, PA66 grade. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation "X Polyamide", 1.6.1998 or ..
|
|||
| Melt Flow |
40
g/10 min <br>@Load 10.0 kg,<br> Temperature 360 °C
|
40
g/10 min <br>@Load 22.0 lb,<br> Temperature 680 °F
|
ISO 1133 |
|
BASF Ultrason S 2010 G4 20% Glass Filled PSU
Ultrason S 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength.
|
|||
| Melt Flow |
40
g/10 min <br>@Load 10.0 kg,<br> Temperature 360 °C
|
40
g/10 min <br>@Load 22.0 lb,<br> Temperature 680 °F
|
ISO 1133 |
|
BASF Ultrason S 3010 PSU
Ultrason S 3010 is an unreinforced, higher viscosity injection molding and extrusion PSU grade, tougher and with improved chemical resistance. It conforms to FDA requirements of 21 CFR 177.1655.
|
|||
| Melt Flow |
40
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
40
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ISO 1133 |
|
Total PPC 10712 Polypropylene, Heterophasic Copolymer
ATOFINA Propylene 10712 is a nucleated and controlled-rheology heterophasic copolymer. PPC 10712 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage.
|
|||
| Melt Flow |
40
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
40
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer (Asia Pacific)
40 MFR LEXAN High Flow Ductile Copolymer
|
|||
| Melt Flow |
40
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
40
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
ASTM D1238 |
|
Samyang Trirex® TH3022N Polycarbonate, High Flow Flame Retardancy
PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.TH3022N is a high flow, flame retardant grade.Applications: LCD TV, Laptop and Monitor..
|
|||
| Melt Flow |
40
g/10 min <br>@Load 5.00 kg,<br> Temperature 190 °C
|
40
g/10 min <br>@Load 11.0 lb,<br> Temperature 374 °F
|
ISO 1133 |
|
Polyplastic TechnoTep A® 65 A Thermoplastic Elastomer, Mineral Filled