Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 446 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 50.0 - 230 °C
122 - 446 °F
Average value: 127 °C Grade Count:89
Overview of materials for Nylon 6, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app..
Deflection Temperature at 1.8 MPa (264 psi) 70.0 - 230 °C
158 - 446 °F
Average value: 191 °C Grade Count:115
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max..
Deflection Temperature at 1.8 MPa (264 psi) 220 - 230 °C
428 - 446 °F
Average value: 228 °C Grade Count:12
Overview of materials for Polyvinyl Dichloride (PVDC)
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC)". Each property range of values reported is minimum and maximum values of ap..
Deflection Temperature at 1.8 MPa (264 psi) 75.0 - 230 °C
167 - 446 °F
Average value: 138 °C Grade Count:17
Overview of materials for Nylon 66, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu..