Material Notes:
STRUKTOL® TPW 613 is a functional lubricant package designed to provide superior filler wetting and dispersion characteristics in a wide range of polymer systems. This product has been engineered to provide significant processing improvements and output rate increases for filled compounds.Applications: STRUKTOL® TPW 613 is recommended for wood-filled polyolefins where improved filler dispersion and surface quality is required.Information provided by Struktol
Physical Properties Metric English Comments
Specific Gravity 1.005 g/cc
1.005 g/cc
Additive Loading 1.0 - 7.0 %
1.0 - 7.0 %
Thermal Properties Metric English Comments
Dropping Point 65.0 - 78.0 °C
149 - 172 °F
Processing Properties Metric English Comments
Shelf Life >= 24.0 Month
>= 24.0 Month
Descriptive Properties Value Comments
Appearance Pastille or beads