Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Mitsubishi Xantar® 18 R Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Molded
Manufacturer Mitsubishi
Trade Name Xantar®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Mitsubishi Xantar® 18 R Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances where quality is a key requirement. The Xantar® range includes: clear and tinted grades for transparent applicationsreinforced materialsFlame retardant and halogen free typeslubricated materials for added wear resistanceMitsubishi Engineering Plastics acquired the Xantar® product line from DSM in 2010.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Water Absorption 0.35 %
0.35 %
Sim. to ISO 62
Viscosity Test 43 cm³/g
43 cm³/g
Limiting Viscosity Number; ISO 1628-4
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
ISO 294-4
Melt Flow 27.6 g/10 min
<br>@Load 1.20 kg,<br> Temperature 300 °C
27.6 g/10 min
<br>@Load 2.65 lb,<br> Temperature 572 °F
Calculated from Volume Flow Rate of 23 cm&lt;sup&gt;3&lt;/sup&gt;/10min.; ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell M 70
70
ISO 2039-2
Tensile Strength, Yield 60.0 MPa
8700 psi
ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
ISO 527-1/-2
Elongation at Yield 6.0 %
6.0 %
ISO 527-1/-2
Tensile Modulus 2.30 GPa
334 ksi
ISO 527-1/-2
Flexural Strength 90.0 MPa
13100 psi
ISO 178
Flexural Modulus 2.40 GPa
348 ksi
ISO 178
Izod Impact, Notched (ISO) 60.0 kJ/m²
<br>@Temperature 23.0 °C
28.6 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 180/4A
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
<br>@Temperature 20.0 °C
36.1 µin/in-°F
<br>@Temperature 68.0 °F
ISO 11359-1/-2
Maximum Service Temperature, Air 125 °C
257 °F
Ball Pressure Temperature; IEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 130 °C
266 °F
ISO 75-1/-2
Vicat Softening Point 145 °C
293 °F
50°C/h 50N; ISO 306
UL RTI, Electrical 130 °C
<br>@Thickness 0.750 mm
266 °F
<br>@Thickness 0.0295 in
UL746B
130 °C
<br>@Thickness 3.00 mm
266 °F
<br>@Thickness 0.118 in
UL746B
UL RTI, Mechanical with Impact 125 °C
<br>@Thickness 0.750 mm
257 °F
<br>@Thickness 0.0295 in
UL746B
130 °C
<br>@Thickness 3.00 mm
266 °F
<br>@Thickness 0.118 in
UL746B
UL RTI, Mechanical without Impact 125 °C
<br>@Thickness 0.750 mm
257 °F
<br>@Thickness 0.0295 in
UL746B
130 °C
<br>@Thickness 3.00 mm
266 °F
<br>@Thickness 0.118 in
UL746B
Flammability, UL94 V-2
<br>@Thickness 1.60 mm
V-2
<br>@Thickness 0.0630 in
IEC 60695-11-10
V-2
<br>@Thickness 0.750 mm
V-2
<br>@Thickness 0.0295 in
IEC 60695-11-10
Oxygen Index 26 %
26 %
ISO 4589-1/-2
Glow Wire Test 800 °C
<br>@Thickness 1.50 mm
1470 °F
<br>@Thickness 0.0591 in
Glow Wire Flammability Index; IEC 60695-2-12
825 °C
<br>@Thickness 1.50 mm
1520 °F
<br>@Thickness 0.0591 in
Glow Wire Ignition Temperature; IEC 60695-2-13
875 °C
<br>@Thickness 3.00 mm
1610 °F
<br>@Thickness 0.118 in
Glow Wire Ignition Temperature; IEC 60695-2-13
960 °C
<br>@Thickness 3.00 mm
1760 °F
<br>@Thickness 0.118 in
Glow Wire Flammability Index; IEC 60695-2-12
Optical Properties Metric English Comments
Transmission, Visible 89 %
89 %
Light Transmittance; ASTM D1003
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
IEC 60093
Dielectric Constant 2.9
<br>@Frequency 1e+6 Hz
2.9
<br>@Frequency 1e+6 Hz
IEC 60250
3.0
<br>@Frequency 100 Hz
3.0
<br>@Frequency 100 Hz
IEC 60250
Dielectric Strength 29.0 kV/mm
737 kV/in
IEC 60243-1
Dissipation Factor 0.00066
<br>@Frequency 100 Hz
0.00066
<br>@Frequency 100 Hz
IEC 60250
0.0092
<br>@Frequency 1e+6 Hz
0.0092
<br>@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 225 V
225 V
IEC 60112
250 - 399 V
250 - 399 V
PLC 2; UL 746A
Descriptive Properties Value Comments
Heat stabilized or stable to heat Yes
High impact or impact modified Yes
Injection molding Yes
Release Agent Yes
Transparent Yes
Without Fillers Yes
Copyright © lookpolymers.com All Rights Reserved