Zoltek Panex 30® High Performance Carbon Yarns

Category Carbon , Carbon Fiber , Other Engineering Material , Composite Fibers
Manufacturer Zoltek
Trade Name Panex 30®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zoltek Panex 30® High Performance Carbon Yarns.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High Performance Carbon YarnsApplications include: High Temperature Packings/Gaskets, Pre-forms for carbon-carbon composites, Polymer Composite Reinforcement
Physical Properties Metric English Comments
Density 1.75 g/cc
0.0632 lb/in³
Component Elements Properties Metric English Comments
Carbon, C 99 %
99 %
Descriptive Properties Value Comments
Denier (g/9000m) 1700
2500
3500
4400
5000
6000
8500
Plies 10
2
3
4
5
6
7
Twist S
Yield, m/kg 1060
1510
1780
2050
2590
3545
5755