Material Notes:
Master Bond Polymer System Supreme 11 features a unique balance of performance properties including both high shear and high peel strengths. This two component adhesive system is formulated to cure at room temperature or more rapidly at elevated temperatures, with a convenient mix ratio of one to one. Master Bond Polymer Adhesive Supreme 11 is suitable for service in a wide temperature range of -100°F to over 300°F.
Physical Properties Metric English Comments
Viscosity 30000 - 40000 cP

@Temperature 23.0 °C
30000 - 40000 cP

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 135 °C
275 °F
Minimum Service Temperature, Air -73.3 °C
-100 °F
Processing Properties Metric English Comments
Cure Time 30.0 - 45.0 min

@Temperature 93.3 °C
0.500 - 0.750 hour

@Temperature 200 °F
1080 - 1440 min

@Temperature 23.0 °C
18.0 - 24.0 hour

@Temperature 73.4 °F
Descriptive Properties Value Comments
Color Code "A" Gray; "B" Tan
Mix Ratio By Weight 100/100
Set-Up Time, minutes 40-50
At Room Temperature