Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Minimum Service Temperature, Air = -100 °F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -73.3 °C
-100 °F
Dielectric Polymers NT-590 Polyimide Film Tape  (discontinued **)
Crosslinked silicone adhesive with polyimide film backing.Features: U.L. recognized class 392°FHigh temperature resistantClean tape removalApplications: For high temperature masking, protecting gol..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Saint-Gobain Chemlam® SGC6-06 Copper Adhesive Tape
Description: Chemlam® Copper SGC6 is fiberglass fabric impregnated with PTFE (polytetrafluoroethylene) dispersion, laminated to PTFE film and coated with high-temperature, pressure-sensitive sili..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Saint-Gobain CHR® 2265-2 Extruded PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Saint-Gobain CHR® 2265-5 Extruded PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Saint-Gobain CHR® G565 Glass Cloth Backing Silicone Adhesive Pressure Sensitive Tape
Description: Glass cloth offers excellent abrasion resistance and mechanical properties, as well as high tensile strength and extreme temperature resistance. Service temperatures range from -100°..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Saint-Gobain CHR® HM350 High Modulus PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Saint-Gobain CHR® M803 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Saint-Gobain CHR® M824 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Saint-Gobain CHR® M827 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Saint-Gobain CHR® SG03-03(R) Premium Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Saint-Gobain CHR® SG03-06(R) Premium Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Saint-Gobain CHR® SG03-10(R) Premium Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Saint-Gobain CHR® SG05-14(R) Premium Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Saint-Gobain CHR® SG35-03(R) Industrial Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Saint-Gobain CHR® SG35-06(R) Industrial Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Saint-Gobain CHR® SG56-03(R) Anti-Static Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Saint-Gobain CHR® A602 Aluminum Foil Backing Silicone Adhesive Pressure Sensitive Tape
Description: Aluminum and copper foil tapes offer high conformability, conductivity, and reflectivity at elevated temperatures. Aluminum is available with a fiberglass laminate for applications requ..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Saint-Gobain CHR® HM650 High Modulus PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Master Bond EP21TDC Toughened, Shock Resistant Two Component Epoxy System
Master Bond Polymer Adhesive EP21TDC is a two component epoxy adhesive for general purpose bonding formulated to cure at room temperature or more rapidly at elevated temperatures, with a one-to-one ..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Master Bond EP21TDC-4 Two Component, Highly Flexible Epoxy System
Master Bond Polymer System EP21TDC-4 is a two component, flexible epoxy resin system for high performance bonding, sealing and coating. It is formulated to cure at ambient temperatures or more quick..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Master Bond EP21TDC-4ND Two component, highly flexibilized epoxy for bonding, sealing and coating
Product Description: Master Bond EP21TDC-4ND is a two component, very flexible epoxy system for high performance bonding, sealing and coating with a non-drip consistency. It has a one to four mix ra..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Master Bond EP46HT-1 Epoxy For Serviceability Up To 600°F
Description: Master Bond EP46HT-1 is a two component epoxy system for high performance structural bonding and sealing suitable for applications where resistance to temperatures from -100°F to +550°..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Master Bond Super Gel 9 Two component urethane modified epoxy gel-like system
Cures at room temperature to form a soft, resilient gel-like system with good dimensional stability. It has excellent optical clarity, convenient to handle, and is easy to retrieve with a sharp kni..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Master Bond Supreme 3HTND-2GT One Part, Toughened, Fast Curing Glob Top Adhesive
Master Bond Polymer System Supreme 3HTND-2GT is a fast curing, toughened one component high performance epoxy adhesive/sealant which meets the growing need for precise positioning and bonding of mic..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Master Bond EP36AN One Part, Toughened, B-Stage Epoxy
Description: Master Bond EP36AN is a unique one component, high performance epoxy for bonding, encapsulation, potting and coating featuring thermal conductivity, electrical insulation and high tempe..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Arlon 99410R015 0.015" Uncured Silicone Rubber with PTFE Coated Fiberglass Substrate
Design/Construction:Interleave: 0.001" FEPSide 1: Unsupported/Uncured Silicone RubberSubstrate: 0.003" PTFE coated FiberglassThis data represents typical values for the production material and sho..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Arlon R36580N008 0.008" ((0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass
Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassAppearance: Grey silicone gumThis data represents typical values for the production material. The dat..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Arlon R33991R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place ..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Arlon R36601A010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate
Description: Generation II Thermabond® NP electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Sty..
Copyright © lookpolymers.com All Rights Reserved