Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Loxim 830 02T V0 Polypropylene Compound, 30% Talc Filled, Flame Retardant

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Talc Filler
Manufacturer Loxim Industries
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Loxim 830 02T V0 Polypropylene Compound, 30% Talc Filled, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Loxim Industries
Physical Properties Metric English Comments
Specific Gravity 1.15 - 1.25 g/cc
1.15 - 1.25 g/cc
ASTM D792
Filler Content 30 %
30 %
Linear Mold Shrinkage 0.0070 - 0.0090 cm/cm
0.0070 - 0.0090 in/in
ASTM D1299
Mechanical Properties Metric English Comments
Tensile Strength at Break 25.0 - 27.0 MPa
3630 - 3920 psi
ASTM D683
Flexural Modulus 2.50 - 3.00 GPa
363 - 435 ksi
ASTM D790
Izod Impact, Notched 0.300 - 0.400 J/cm
0.562 - 0.749 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 - 115 °C
230 - 239 °F
ASTM D1525, HDT Method B
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Users viewing this material also viewed the following: