Thermal Properties Metric English Comments
Minimum Service Temperature, Air -73.3 °C
-100 °F
Arlon Thermabond® R37340X008 Primerless Electronic Adhesive  (discontinued **)
Liner: 1 mil FEP; Product: uncured Silicone Rubber; Carrier: 3 mil PTFE coated fiberglas
Minimum Service Temperature, Air -73.3 °C
-100 °F
Dielectric Polymers NT-590DL Protective Film  (discontinued **)
Crosslinked silicone adhesive with polyimide film backing.Features: U.L. recognized Class 392°FHigh temperature resistantDie cut disks/shapes remove easily from linerClean tape removalApplications:..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Garlock 706 Compressed Inorganic Fiber Gasketing, Nitrile Binder
Inorganic fibers with a nitrile binder.Inorganic, asbestos-free fibers offer superior performance in saturated and superheated steamThermally stable fibers retain effective seal even during thermal ..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Garlock 9900 Compressed Graphite Fiber Gasketing, Nitrile Binder
Graphite fibers with a nitrile binder.Graphite fiber gasketing withstands extreme temperatures and pressures, as well as many chemicalsPassed Garlock Fire tests, and is ABS Fire Safe Type ApprovedLo..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Saint-Gobain Chemlam® SGC6-06 Copper Adhesive Tape
Description: Chemlam® Copper SGC6 is fiberglass fabric impregnated with PTFE (polytetrafluoroethylene) dispersion, laminated to PTFE film and coated with high-temperature, pressure-sensitive sili..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Saint-Gobain CHR® 2905-10R Glass Cloth Backing Silicone Adhesive Pressure Sensitive Tape
Description: Glass cloth offers excellent abrasion resistance and mechanical properties, as well as high tensile strength and extreme temperature resistance. Service temperatures range from -100°..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Saint-Gobain CHR® C Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: FEP film is used for applications requiring optical clarity, quick release, and abrasion resistance. FEP film applications include high temperature coil and capacitor wrapping, composit..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Saint-Gobain CHR® G565 Glass Cloth Backing Silicone Adhesive Pressure Sensitive Tape
Description: Glass cloth offers excellent abrasion resistance and mechanical properties, as well as high tensile strength and extreme temperature resistance. Service temperatures range from -100°..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Saint-Gobain CHR® M832 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Saint-Gobain CHR® SG06-03(R) Premium Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Saint-Gobain CHR® SG16-10(R) High Performance Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Saint-Gobain CHR® SG16-14(R) High Performance Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Saint-Gobain CHR® SG25-05(R) Primary Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Saint-Gobain CHR® SG35-05(R) Industrial Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Saint-Gobain CHR® SG56-05(R) Anti-Static Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Saint-Gobain CHR® SGB6-10(R) CHEMLAM Brown Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Saint-Gobain CHR® T903 TRIFOIL™ PTFE/Aluminum Foil Backing Silicone Adhesive Pressure Sensitive Tape
Description: Aluminum and copper foil tapes offer high conformability, conductivity, and reflectivity at elevated temperatures. Aluminum is available with a fiberglass laminate for applications requ..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Saint-Gobain CHR® C663 Paper Backing Silicone Adhesive Pressure Sensitive Tape
Description: Paper tapes are designed to provide high temperature and excellent solvent resistance for wave soldering, printed circuit board masking, and hot air leveling applications. Service tempe..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Saint-Gobain CHR® T Skived PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Arlon CP-499CA Bulk Compound
This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Arlon R30370A008 0.008" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 0.001" FEP FilmSide 1: Unsupported/Uncured Silicone RubberSubstrate: 0.003" PTFE coated FiberglassThis data represents typical values for the production material a..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Arlon Thermabond® 99000W008 Silicone Rubber/Fiberglass Laminate
Low outgassing, thermally conductive, electrically insulating, Thermabond®. Bonds with primer. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass.
Minimum Service Temperature, Air -73.3 °C
-100 °F
Arlon Thermabond® 99950N015 Silicone Rubber/Fiberglass Laminate
Electrically conductive, Thermabond®. primerless. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass.
Minimum Service Temperature, Air -73.3 °C
-100 °F
Arlon Thermabond® R36300W008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: Low Outgassing, Thermally Conductive, Electrically Insulating, Thermabond® Bonds without primerRecommended Primers: Dow Corning S2260Design/Construction: Liner: FEP Product: Uncured S..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Arlon Thermabond® R36300W015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Primers: Dow Corning S2260Appearance: White silicone gumThis data represents typical val..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Arlon Thermabond® T20 (99710W015) 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: 15 mil thick Thermabond® T20 electrically insulating electronic adhesive.Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Pri..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Arlon Thermabond® T-20 NP (99770W015) 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: 15 mil Primerless Thermabond®. T-20 NP. Thermally conductive, electrically insulating electronic adhesive. Bonds with primer.Design/Construction:Liner: FEPProduct: Uncured Silicone Rub..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Arlon R33991R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place ..
Minimum Service Temperature, Air -73.3 °C
-100 °F
Master Bond EP39MHT Two Component, Room Temperature Curing Epoxy Resin System
Master Bond Polymer System EP39MHT is a low viscosity, two component, epoxy resin system for high performance potting, encapsulation, sealing and bonding. It cures readily at ambient temperatures to..