Material Notes:
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Isotropic shrinkage characteristics.Control disks, cams, sliding elements and other duty parts.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
ISO 1183
Water Absorption <= 1.0 %
<= 1.0 %
23°C/24h
Linear Mold Shrinkage 0.010 - 0.015 cm/cm
0.010 - 0.015 in/in
Mechanical Properties Metric English Comments
Tensile Stress 86.0 MPa
12500 psi
Elongation at Yield 5.0 %
5.0 %
Modulus of Elasticity 3.00 GPa
435 ksi
Flexural Strength 130 MPa
18900 psi
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
flatwise; ISO 179 1fU
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 90.0 °C
194 °F
110 °C
230 °F
short term
Electrical Properties Metric English Comments
Surface Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Insulation Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Processing Properties Metric English Comments
Processing Temperature 290 °C
554 °F
mass temp
Nozzle Temperature 280 - 300 °C
536 - 572 °F
Zone 1 290 - 310 °C
554 - 590 °F
Zone 2 290 - 310 °C
554 - 590 °F
Zone 3 290 - 310 °C
554 - 590 °F
Mold Temperature 90.0 - 120 °C
194 - 248 °F
Drying Temperature 75.0 °C

@Time 21600 - 57600 sec
167 °F

@Time 6.00 - 16.0 hour
Dehumidifying dryer
105 °C

@Time 14400 - 21600 sec
221 °F

@Time 4.00 - 6.00 hour
Vacuum Dryer
Descriptive Properties Value Comments
Color dark grey