Polymer Property : Zone 2 = 290 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-7004 Polyamide 66, with glass fiber and carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically ..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-7789/EG Polyamide 66, with carbon fiber, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Antistatic.High dimensi..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-7791 Polyamide 66, with carbon fiber, PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-8490 Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.High dimensionally stab..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-8491 Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.High dimensionally stab..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-RG 1 Polyamide 66, with PAN-carbon fiber, RG-standard
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 50/CF/7/GF/20/TF/10/BK Polycarbonate, with carbon fiber, glass fiber and PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 50/GF/10/TF/18/SI/2/GY5 Polycarbonate, with glass fiber, PTFE, lubricant modified
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 50-3019 Polycarbonate, with glass fiber and PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts, even at elevated te..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 50-7154/V0 Polycarbonate, with carbon fiber, low-warpage
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Reduced moment of inertia compared with me..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 50-8300 Polycarbonate, with PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts, even at elevated te..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 50-8479/BL Polycarbonate, unreinforced
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Isotropic shrinkage characteristics.Reduced moment of inertia ..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1/CF/20/TF/15 Polyamide 66, with carbon fiber and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1/CF/20/TF/5 Polyamide 66, with carbon fiber and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1/CF/30 Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-0866 Polyamide 66, with aramid reinforcement, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Low warpage.Improved heat resistance.Control disks, cams, sliding elements and other duty parts..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-1119 VP Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-1119-1 Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-7139-1 Polyamide 66, with aramid reinforcement and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Improved heat resistance.Control disks, cams, sliding elements and o..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-7817 Polyamide 66, with carbon fiber, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrical..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-7830 Polyamide 66, with PTFE, lubricant modified, improved wear resistance, high viscosity
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-7956 Polyamide 66, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-7984 Polyamide 66, with aramid reinforcement and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Improved heat resistance.Control disks, cams, sliding elements and o..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 50/CF/5/GF/10 Polycarbonate, with carbon fiber and glass fiber
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi..
Zone 2 290 - 330 °C
554 - 626 °F
Solvay Specialty Polymers Hyflon® MFA® 1041 Perfluoropolymer
Hyflon® MFA 1041 is a high extrusion speed resin specifically designed for insulation for plenum-rated LAN cables. MFA 1041 delivers superior electrical performance in addition to its excellent f..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-8130 Polyamide 66, with carbon fiber, aramid reinforcement and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved wear behaviour, low warpage.Emergency running property, for highest tribologic needs.R..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-8228 Polyamide 66, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..