Engineered Syntactic Systems SF-30 Subsea Syntactic Void Filler

Category Polymer , Thermoset , Epoxy
Manufacturer Engineered Syntactic Systems
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Engineered Syntactic Systems SF-30 Subsea Syntactic Void Filler.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SF-30 is a low cost, low density syntactic formulated to serve as a void filler for shallow water subsea applications. The material is provided as a three-part kit that is mixed and poured into any freeflood cavity or void. The mix is allowed to cure at room temperature to form a solid syntactic material that will withstand repeated ocean excursions to depths of 1,500 feet. The easily cast system is provided in three parts; two resin components and a solid filler. The two resin components are mixed together, followed by the glass bubble filler. When the three materials are uniformly mixed, the moderate viscosity combination may be poured into its desired location. Initial cure will occur over a twenty four hour period at ambient temperatures, (50°F - 90 °F), providing a solid, lightweight article which is ready for any secondary operation such as machining, finishing or painting. Full cure will take place after 7 – 10 days. The cured material will provide an average of 34 pounds of buoyancy per cubic foot in seawater.
Physical Properties Metric English Comments
Density <= 0.481 g/cc
<= 0.0174 lb/in³
Water Absorption <= 3.0 %

@Time 86400 sec
<= 3.0 %

@Time 24.0 hour
at 1500 ft.depth
Mechanical Properties Metric English Comments
Compressive Strength >= 14.5 MPa
>= 2100 psi
Compressive Modulus >= 0.896 GPa
>= 130 ksi
Hydrostatic Design Basis 8.27 MPa
1200 psi
Hydrostatic Crush Strength (2700 feet)
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
from manufacture date