Polymer Property : Drying Temperature = 167 °F Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Drying Temperature 75.0 °C

@Time 21600 - 57600 sec
167 °F

@Time 6.00 - 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1-7789/EG Polyamide 66, with carbon fiber, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Antistatic.High dimensi..
Drying Temperature 75.0 °C

@Time 21600 - 57600 sec
167 °F

@Time 6.00 - 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1-7791 Polyamide 66, with carbon fiber, PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh..
Drying Temperature 75.0 °C

@Time 21600 - 57600 sec
167 °F

@Time 6.00 - 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1-7985 Polyamide 66, with aramid reinforcement and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Improved heat resistance.Control disks, cams, sliding elements and o..
Drying Temperature 75.0 °C

@Time 21600 - 57600 sec
167 °F

@Time 6.00 - 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1-8064 Polyamide 66, with carbon fiber, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Antistatic.High dimensi..
Drying Temperature 75.0 °C

@Time 21600 - 57600 sec
167 °F

@Time 6.00 - 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1-8218 Polyamide 66, with carbon fiber, toughness-modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; impact resistance.Reduced moment of inertia compared with metal parts.Elec..
Drying Temperature 75.0 °C

@Time 21600 - 57600 sec
167 °F

@Time 6.00 - 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1-8379 Polyamide 66, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Drying Temperature 75.0 °C

@Time 21600 - 57600 sec
167 °F

@Time 6.00 - 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1-8501 Polyamide 66, with glass fiber, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.dynamic st..
Drying Temperature 75.0 °C

@Time 36000 - 57600 sec
167 °F

@Time 10.0 - 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 3/CF/10/BK Polyamide 6, with carbon fiber
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable..
Drying Temperature 75.0 °C

@Time 36000 - 57600 sec
167 °F

@Time 10.0 - 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 3/CF/30 Polyamide 6, with carbon fiber
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable..
Drying Temperature 75.0 °C

@Time 36000 - 57600 sec
167 °F

@Time 10.0 - 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 3-7723/ EG Polyamide 6, with carbon fiber, high viscosity
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressAntistatic.Handles, levers, rolle..
Drying Temperature 75.0 °C

@Time 36000 - 57600 sec
167 °F

@Time 10.0 - 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 3-8269 Polyamide 6, with basalt fiber
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts; impact resistance.dynamic stressReduced moment of inertia compared with metal parts.Be..
Drying Temperature 75.0 °C

@Time 36000 - 57600 sec
167 °F

@Time 10.0 - 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 3-8277 Polyamide 6, unreinforced
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce..
Drying Temperature 75.0 °C

@Time 36000 - 57600 sec
167 °F

@Time 10.0 - 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 3-8351 Polyamide 6, with carbon fiber
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated el..
Drying Temperature 75.0 °C

@Time 21600 - 36000 sec
167 °F

@Time 6.00 - 10.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 6-7833 Polyamide 12, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Low waterabsorbtion, for dimensional stable precision parts.Isotropic sh..
Drying Temperature 75.0 °C

@Time 21600 - 36000 sec
167 °F

@Time 6.00 - 10.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 6-8395 Polyamide 12, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Especially suitable at dynamic stress situations.Electrically conductive, s..
Drying Temperature 75.0 °C

@Time 7200 - 28800 sec
167 °F

@Time 2.00 - 8.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 80/TF/18/SI/2/BK Polyacetal-copolymer, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
Drying Temperature 75.0 °C

@Time 7200 - 28800 sec
167 °F

@Time 2.00 - 8.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 80-7666/GY Polyacetal-copolymer, with glass fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
Drying Temperature 75.0 °C

@Time 7200 - 28800 sec
167 °F

@Time 2.00 - 8.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 80-7705 Polyacetal-copolymer, with carbon fiber, aramid reinforcement and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Suitable for discharging of st..
Drying Temperature 75.0 °C

@Time 7200 - 28800 sec
167 °F

@Time 2.00 - 8.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 80-7752 Polyacetal-copolymer, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita..
Drying Temperature 75.0 °C

@Time 7200 - 28800 sec
167 °F

@Time 2.00 - 8.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 80-8162 Polyacetal-copolymer, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
Drying Temperature 75.0 °C

@Time 7200 - 28800 sec
167 °F

@Time 2.00 - 8.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 80-8387 Polyacetal-copolymer, unreinforced
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Isotropic shrinkage characteristics.Strong, stiff parts.Impact resistance.Control disks, cams, ..
Drying Temperature 75.0 °C

@Time 21600 - 57600 sec
167 °F

@Time 6.00 - 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1-0889-5 Polyamide 66, with carbon fiber and glass fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically ..
Drying Temperature 75.0 °C

@Time 21600 - 57600 sec
167 °F

@Time 6.00 - 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1-1119 VP Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Drying Temperature 75.0 °C

@Time 21600 - 57600 sec
167 °F

@Time 6.00 - 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1-7180/EG Polyamide 66, with carbon fiber, PTFE, lubricant modified, high viscosity, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Drying Temperature 75.0 °C

@Time 7200 - 28800 sec
167 °F

@Time 2.00 - 8.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 80-7919 Polyacetal-copolymer, with PTFE, easy flowing
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
Drying Temperature 75.0 °C

@Time 36000 - 57600 sec
167 °F

@Time 10.0 - 16.0 hour
Dehumidifying dryer
Lehmann & Voss Nylatron® MR 2007 Polyamide 6, with mineral filler
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Low warpage.Isotropic shrinkage characteristics.Information provided by Lehmann & Voss & Co.KG
Drying Temperature 75.0 °C

@Time 21600 - 57600 sec
167 °F

@Time 6.00 - 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1/XCF/25 Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Drying Temperature 75.0 °C

@Time 21600 - 57600 sec
167 °F

@Time 6.00 - 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1-0890 Polyamide 66, with carbon fiber, low-warpage, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Stiff parts, low coefficient of expansion, low viscose, anisotropic.Reduced moment of inertia c..
Drying Temperature 75.0 °C

@Time 21600 - 57600 sec
167 °F

@Time 6.00 - 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1-7233-1 Polyamide 66, with glass fiber, PTFE, lubricant modified, silicone-free
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Bearings, ..
Drying Temperature 75.0 °C

@Time 21600 - 57600 sec
167 °F

@Time 6.00 - 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1-8228 Polyamide 66, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..