Ensinger Tecapeek® XP-97 Compression Molded PEEK Compound, 30% Graphite Filled

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer Ensinger
Trade Name Tecapeek®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecapeek® XP-97 Compression Molded PEEK Compound, 30% Graphite Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in lower amounts of scrap, uniform physical properties and fewer molded-in stresses.TECAPEEK is a high-perfomance engineering thermoplastic. This semi-crystalline material has a balance of high temperature mechanical properties, chemical and steam resistance, superior wear properties and processability which makes it unique.Applications Include:Bearings and BushingsDown-hole instrumentationWear RingsBall Valve SeatsElectrical ComponentsBack-up and V-RingsPiston Rings and Rider BandsInformation provided by Ensinger Special Polymers, Inc.
Physical Properties Metric English Comments
Density 1.53 g/cc
0.0553 lb/in³
ASTM D792
Filler Content 30 %
30 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 92
92
ASTM D785
Hardness, Shore D 83
83
ASTM D2240
Tensile Strength 55.2 MPa
8000 psi
ASTM D638
Elongation at Break 1.1 %
1.1 %
ASTM D638
Tensile Modulus 9.65 GPa
1400 ksi
ASTM D638
Flexural Strength 84.1 MPa
12200 psi
ASTM D790
Flexural Modulus 6.89 GPa
1000 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 343 °C
649 °F
DSC
Descriptive Properties Value Comments
Color Black