| Category | Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded | 
| Manufacturer | Ineos ABS | 
| Trade Name | Lustran® | 
| Port | Shanghai port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Ineos ABS Lustran® Elite HH 1891.pdf  | 
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Density | 1.05 g/cc | 0.0379 lb/in³ | |
| Melt Flow | 7.2           g/10 min @Load 10.0 kg, Temperature 220 °C | 7.2           g/10 min @Load 22.0 lb, Temperature 428 °F | cm³/10 min. | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Tensile Strength, Yield | 42.9 MPa | 6220 psi | |
| Elongation at Break | 35 % | 35 % | Nominal | 
| Elongation at Yield | 4.0 % | 4.0 % | |
| Tensile Modulus | 2.05 GPa | 297 ksi | |
| Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | |
| 0.590           J/cm² @Temperature -30.0 °C | 2.81           ft-lb/in² @Temperature -22.0 °F | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| CTE, linear, Parallel to Flow | 79.0           µm/m-°C @Temperature 20.0 °C | 43.9           µin/in-°F @Temperature 68.0 °F | |
| Deflection Temperature at 0.46 MPa (66 psi) | 101 °C | 214 °F | |
| Deflection Temperature at 1.8 MPa (264 psi) | 86.0 °C | 187 °F | |
| Vicat Softening Point | 106 °C | 223 °F | 50°C/h 50N | 
| Processing Properties | Metric | English | Comments | 
|---|---|---|---|
| Melt Temperature | 250 °C | 482 °F | Injection Molding | 
| Mold Temperature | 60.0 °C | 140 °F | Injection Molding | 
| Injection Velocity | 200 mm/sec | 7.87 in/sec | |
| Injection Pressure | 55.0 MPa | 7980 psi |