Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 218G V33 Black 41N PA66, 33% glass fiber, DRY.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: TECHNYL® A 218G V33 Black 41N is a polyamide 66, reinforced with 33% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This product has been specially designed to improve its resistance to automotive cooling liquids, increasing lifetime of parts in permanent contact with such a liquids. It is also specially formulated to offer a good surface aesthetics.Available in: North AmericaRegulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.Applications: TECHNYL A 218G V33 Black 41N is particularly recommended for the injection molding of gun stocks and frames, as well as parts in permanent contact with cooling liquids in transport vehicles such as: cooling and heating radiator systems, tank headers, thermostat components, inlet and outlet pipes.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
ISO 1183/A
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
Linear Mold Shrinkage, Transverse 0.010 cm/cm
0.010 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 174 MPa
25200 psi
ISO 527 Type 1A
Elongation at Break 2.9 %
2.9 %
ISO 527 Type 1A
Tensile Modulus 8.50 GPa
1230 ksi
ISO 527 Type 1A
Flexural Strength 264 MPa
38300 psi
ISO 178
Flexural Modulus 8.70 GPa
1260 ksi
ISO 178
Izod Impact, Notched (ISO) 9.80 kJ/m²
4.66 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched 7.20 J/cm²
34.3 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.870 J/cm²
4.14 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
ISO 75/Af
Processing Properties Metric English Comments
Feed Temperature 255 - 265 °C
491 - 509 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Compression Zone 265-275°C
Mixing Zone 275-280°C