Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3A Composites Core Materials AIREX® T92.200 Easy Processing Structural Foam

Category Other Engineering Material , Composite Core Material , Polymer , Thermoplastic
Manufacturer 3A Composites Core Materials
Trade Name AIREX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3A Composites Core Materials AIREX® T92.200 Easy Processing Structural Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable, UV resistant and has negligible water absorption. It is thermally stable during high temperature processing and post curing without after expansion or out-gassing. T92 is designed for easy use with all resin systems and processing technologies. AIREX® T92 is ideally suited as a core material for a wide variety of lightweight sandwich structures subjected to static and dynamic loads and/or exposed to elevated temperatures during manufacturing.CharacteristicsEasy to process with all types of resin and lamination processesHigh process temperature up to 150°C (302°F)Excellent fatigue strengthHigh compression and shear propertiesVery low variance of mechanical propertiesExcellent chemical stabilityGood adhesion (skin-to-core bond)Excellent long term thermal stability up to 100°C (212°F)No water absorptionNo after expansion, no out-gassingApplicationsWind energy: Blades (shear webs & shells), nacellesMarine: Hulls, decks, superstructures, bulkheads, transoms, interiors stringersIndustrial: Cover, containers, local reinforcements, x-ray tables, sporting goods
Physical Properties Metric English Comments
Density 0.210 g/cc
0.00759 lb/in³
average; ISO 845
0.200 - 0.220 g/cc
0.00723 - 0.00795 lb/in³
typical range; ISO 845
Mechanical Properties Metric English Comments
Tensile Strength >= 2.50 MPa
>= 363 psi
perpendicular to plane; ASTM C297
3.10 MPa
450 psi
average; perpendicular to plane; ASTM C297
Elongation at Break >= 4.0 %
>= 4.0 %
shear; ISO 1922
6.0 %
6.0 %
average; shear; ISO 1922
Tensile Modulus >= 0.190 GPa
>= 27.6 ksi
perpendicular to plane; ASTM C297
0.230 GPa
33.4 ksi
average; perpendicular to plane; ASTM C297
Compressive Strength >= 3.20 MPa
>= 464 psi
perpendicular to plane; ISO 844
3.50 MPa
508 psi
average; perpendicular to plane; ISO 844
Compressive Modulus >= 0.150 GPa
>= 21.8 ksi
perpendicular to plane; DIN 53421
0.180 GPa
26.1 ksi
average; perpendicular to plane; DIN 53421
Shear Modulus >= 0.0450 GPa
>= 6.53 ksi
ASTM C393
0.0500 GPa
7.25 ksi
average; ASTM C393
Shear Strength >= 1.60 MPa
>= 232 psi
ISO 1922
2.00 MPa
290 psi
average; ISO 1922
Thermal Properties Metric English Comments
Thermal Conductivity 0.0410 W/m-K
0.285 BTU-in/hr-ft²-°F
ISO 8301
Copyright © lookpolymers.com All Rights Reserved