Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 79.0 µm/m-°C

@Temperature 20.0 °C
43.9 µin/in-°F

@Temperature 68.0 °F
Ineos ABS Lustran® Elite HH 1891
Key Features:UnfilledHeat stabilized or stable to heatSuitable processing methods:Injection molding
CTE, linear, Parallel to Flow 79.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
43.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP DL004 PC (Europe-Africa-Middle East)
LNP* LUBRICOMP* DL004 is a compound based on Polycarbonate resin containing PTFE. Added features include Internally Lubricated.
CTE, linear, Parallel to Flow 79.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
43.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP ZL003 PPE+PS (Europe-Africa-Middle East)
LNP* LUBRICOMP* ZL003 is a compound based on PPE+PS Blend resin containing PTFE. Added features include Internally Lubricated.
CTE, linear, Parallel to Flow 79.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
43.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP MX95318 PP
LNP* THERMOCOMP* MX95318 is a compound based on Polypropylene containing Proprietary Filler(s).
CTE, linear, Parallel to Flow 79.0 µm/m-°C

@Temperature 20.0 °C
43.9 µin/in-°F

@Temperature 68.0 °F
ISO data
Styron Magnumâ„¢ 275 ABS, Low Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
CTE, linear, Parallel to Flow 79.0 µm/m-°C

@Temperature 20.0 °C
43.9 µin/in-°F

@Temperature 68.0 °F
ISO data
Styron Magnumâ„¢ 348 ABS, Low Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
CTE, linear, Parallel to Flow 79.0 µm/m-°C

@Temperature 20.0 °C
43.9 µin/in-°F

@Temperature 68.0 °F
ISO data
Styron Magnumâ„¢ 541 ABS, High Impact
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
CTE, linear, Parallel to Flow 79.0 µm/m-°C

@Temperature 20.0 °C
43.9 µin/in-°F

@Temperature 68.0 °F
ISO data
Styron Magnumâ„¢ 585 ABS
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
CTE, linear, Parallel to Flow 79.0 µm/m-°C

@Temperature 20.0 °C
43.9 µin/in-°F

@Temperature 68.0 °F
ISO data
Styron Magnumâ„¢ 8325 ABS, Sheet Coextrusion Grade
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
CTE, linear, Parallel to Flow 79.0 µm/m-°C

@Temperature 20.0 °C
43.9 µin/in-°F

@Temperature 68.0 °F
ISO data
Styron Magnumâ„¢ FG960 ABS, High Impact
MAGNUM ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS ..
CTE, linear, Parallel to Flow 79.0 µm/m-°C

@Temperature 20.0 °C
43.9 µin/in-°F

@Temperature 68.0 °F
ISO data
Styron Magnumâ„¢ PG914 ABS, High Impact
MAGNUM ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS ..
CTE, linear, Parallel to Flow 79.0 µm/m-°C

@Temperature 20.0 °C
43.9 µin/in-°F

@Temperature 68.0 °F
ISO data
Styron Magnumâ„¢ 341 ABS, Low Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..