Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ISO 1183 |
Moisture Absorption | 0.900 % | 0.900 % | ISO 62 |
Maximum Moisture Content | 0.10 | 0.10 | Karl Fischer |
Linear Mold Shrinkage, Flow | 0.0030 cm/cm @Temperature 80.0 °C |
0.0030 in/in @Temperature 176 °F |
60x60x2 mm; ISO 294-4 |
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm @Temperature 80.0 °C |
0.0070 in/in @Temperature 176 °F |
60x60x2 mm; ISO 294-4 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore D | 93 | 93 | [N/mm<sup>2<sup>]; ISO 7619 |
Tensile Strength | 173 MPa | 25000 psi | 50 mm/min; ISO 527-1,-2 |
Elongation at Break | 3.3 % | 3.3 % | 50 mm/min; ISO 527 |
Tensile Modulus | 9.70 GPa | 1410 ksi | 1 mm/min; ISO 527-1,-2 |
Flexural Strength | 265 MPa | 38400 psi | 5 mm/min; ISO 178 |
Flexural Modulus | 8.53 GPa | 1240 ksi | 5 mm/min; ISO 178 |
Izod Impact, Notched (ISO) | 11.5 kJ/m² | 5.47 ft-lb/in² | ISO 180-1A |
Charpy Impact Unnotched | 9.10 J/cm² @Temperature 23.0 °C |
43.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
Charpy Impact, Notched | 1.20 J/cm² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1A |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 220 °C | 428 °F | 10°C/min; ISO 11357-1,-3 |
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | ISO 75-1,-2 |
Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | ISO 75-1,-2 |
Flammability, UL94 | HB @Thickness 1.60 mm |
HB @Thickness 0.0630 in |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 270 - 290 °C | 518 - 554 °F | ISO 294 |
Mold Temperature | 80.0 - 120 °C | 176 - 248 °F | ISO 294 |
Drying Temperature | 80.0 °C | 176 °F | |
Dry Time | 2.00 - 6.00 hour | 2.00 - 6.00 hour |