| Category | Metal , Nonferrous Metal , Copper Alloy |
| Manufacturer | Goodfellow |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Goodfellow Phosphor Bronze.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 8.90 g/cc | 0.322 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Brinell | 80 - 225 | 80 - 225 | |
| Tensile Strength at Break | 320 - 740 MPa | 46400 - 107000 psi | |
| Elongation at Break | <= 60 % | <= 60 % | |
| Tensile Modulus | 90.0 - 120 GPa | 13100 - 17400 ksi | |
| Shear Strength | 250 - 430 MPa | 36300 - 62400 psi | |
| Izod Impact, Unnotched | 0.620 J/cm | 1.16 ft-lb/in | Notch Status Unknown |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 17.0 µm/m-°C @Temperature 20.0 - 100 °C |
9.44 µin/in-°F @Temperature 68.0 - 212 °F |
|
| Thermal Conductivity | 50.0 - 75.0 W/m-K | 347 - 521 BTU-in/hr-ft²-°F | |
| Melting Point | 900 - 1050 °C | 1650 - 1920 °F | |
| Solidus | 900 °C | 1650 °F | |
| Liquidus | 1050 °C | 1920 °F |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Copper, Cu | 94 % | 94 % | |
| Tin, Sn | 6.0 % | 6.0 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 0.0000110 - 0.0000160 ohm-cm | 0.0000110 - 0.0000160 ohm-cm | Temperature Coefficient of 0.0006 to 0.0007/K |