Buckeye Polymers BP Flex D7030 UC85 TPO

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer Buckeye Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Buckeye Polymers BP Flex D7030 UC85 TPO.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Bumpers, Air damsTPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a wide service range from -20 degrees C to 120 degrees C, high tear resistance, low density, and good paintability.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955
Melt Flow 11 g/10 min
11 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 52
52
ASTM D2240
Tensile Strength, Ultimate 22.1 MPa
3210 psi
ASTM D638
Flexural Modulus 0.800 GPa
116 ksi
ASTM D790
Gardner Impact NB
NB
Tear Strength 96.4 kN/m
550 pli
ASTM D624