Kazanorgsintez 11503-070 UUP Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Kazanorgsintez
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kazanorgsintez 11503-070 UUP Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Production Method: LDPE is produced by high pressure ethylene polymerization in tubular reactors. Application: Designed for packaging and production of products designed for food contact, toy production, and medicine containers.Information Provided by Kazanorgsintez
Physical Properties Metric English Comments
Density 0.917 - 0.919 g/cc
0.0331 - 0.0332 lb/in³
Melt Flow 7.0 g/10 min
7.0 g/10 min
±15%
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 9.32 MPa
>= 1350 psi
Elongation at Break >= 450 %
>= 450 %
Tear Strength Test >= 9.8
>= 9.8
MPa
Descriptive Properties Value Comments
Amount of impurities [pcs] 10
2nd Quality
2
Superior Quality
5
Premium Quality
Extractable Substance Weight Content (%) 0.8