Polymer Property : Tensile Modulus = 225 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 1.55 GPa
225 ksi
STN EN ISO 527-2
Plastcom PLASTALEN® PC 69 T 10 003/1M Polypropylene reinforced with mineral filler
Modified PP copolymer for injection molding with the content of 10% mineral filler. Application in all automotive industry. Delivered in black.Information Provided by Plastcom spol. s r.o.
Tensile Modulus 1.55 GPa
225 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne LubriOne™ PC-20GF/15T Polycarbonate (PC)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Tensile Modulus 1.55 GPa
225 ksi
ISO 527-1/-2
Quadrant EPP Borotron® HM PE-HMW + boron based additive (ISO Data)
Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very su..
Tensile Modulus 1.55 GPa
225 ksi
Radici Radilon® A ECP3808 (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Tensile Modulus 1.55 GPa
225 ksi
ASTM D638
Fiberfil® J-60/GB/20 Polypropylene Homopolymer, 20% Glass beads
Information provided by FIBERFIL Engineered Plastics
Tensile Modulus 1.55 GPa
225 ksi
DIN 53457
Isoflon PA 12 Polyamide 12
General use for mechanical partsGood heat resistanceEasy to useInformation provided by Isoflon.
Tensile Modulus 1.55 GPa
225 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-LOY A3000TXB ABS
LNP* STAT-LOY* A3000TXB is a compound based on ABS resin. Added features of this material include: Antistatic, Transparent, Formulated with FDA Food Contact Additives and Bioassessed to ISO 10993...
Tensile Modulus 1.55 GPa
225 ksi
1mm/min; ISO 527
Styrolution Styrolux 684D SBC
Styrolux 684D is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion, and thermoforming. It offers an outstanding combination of crystal clarity and..
Tensile Modulus 1.55 GPa
225 ksi
ISO 527
Borealis Daploy™ WF420HMS High Melt Strength Polypropylene for Extrusion Coating
Daploy WF420HMS resin is a propylene-based, structurally isomeric polymer, which combines significantly increased melt strength with largely drawability of the polymer melt. Thus, the material is g..
Tensile Modulus 1.55 GPa
225 ksi
ISO 527-2
Total PPH 4069 Polypropylene Homopolymer, Fiber
Polypropylene PPH 4069 is a homopolymer polypropylene with a Melt Flow index of 4 g/10 min.Polypropylene PPH 4069 is intended for extrusion of high tenacity staple fibers for non-woven applications...
Tensile Modulus 1.55 GPa
225 ksi
ISO 527-2
Total PPH 7060 Polypropylene, Homopolymer
ATOFINA Polypropylene PPH 7060 is homopolymer.ApplicationATOFINA Polypropylene PPH 7060 is intended for the injection molding of packaging containers, toys, domestic appliances, garden furniture and..
Tensile Modulus 1.55 GPa
225 ksi
ISO 527-2
Total PPH 7062 Polypropylene, Homopolymer
ATOFINA Polypropylene PPH 7062 is an antistatic homopolymer.ApplicationATOFINA Polypropylene PPH 7062 is intended for injection molding applications of boxes, closures and household articles. Inform..
Tensile Modulus 1.55 GPa
225 ksi
ISO 527-2
Total PPH 8069 Polypropylene, Homopolymer
ATOFINA Polypropylene PPH 8069 is homopolymer.ApplicationATOFINA Polypropylene PPH 8069 has been developed for the production of staple fibers for non-wovens. PPH 8069 has a special anti gas-fading..
Tensile Modulus 1.55 GPa
225 ksi
1mm/min; ISO 527-2
Borealis BS4641 High Density Polyethylene
BS4641 is a bimodal high-density polyethylene homopolymer. Because of its excellent organoleptic properties, this grade is especially suitable for blow molding of bottles for food applications. App..
Tensile Modulus 1.55 GPa
225 ksi
ASTM D638
Eastman Tritan MX710 Copolyester
Eastman Tritan Copolyester MX710 is an amorphous product with excellent appearance and clarity. Eastman Tritan Copolyester MX710 has many outstanding features that include excellent toughness, hydr..
Tensile Modulus 1.55 GPa
225 ksi
ASTM D638
Eastman Tritan MX711 Copolyester
Eastman Tritan Copolyester MX711 is an amorphous product with excellent appearance and clarity. Eastman Tritan MX711 contains a mold release derived from vegetable based sources. Eastman Tritan Co..
Tensile Modulus 1.55 GPa
225 ksi
ASTM D638
Eastman Tritan TX1000 Copolyester
Eastman Tritan TX1000 is an amorphous copolyester with excellent appearance and clarity. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistanc..
Tensile Modulus 1.55 GPa
225 ksi
ASTM D638
Eastman Tritan TX1001 Copolyester
Eastman Tritan TX1001 is an amorphous copolyester with excellent appearance and clarity. Eastman Tritan TX1001 contains a mold release derived from vegetable based sources. Its most outstanding fe..
Tensile Modulus 1.55 GPa
225 ksi
ASTM D638
CPC - Vycom FLAMETEC™ KYTEC® PVDF
Kytec® PVDF, the homopolymer of 1, 1-difluoroethene, is a tough engineering thermoplastic that offers a unique balance of properties. Kytec has the characteristic stability of fluoropolymers when e..
Tensile Modulus 1.55 GPa
225 ksi
ISO 527-2
Domo 1100N Polypropylene Homopolymer
Information provided by Domo.
Tensile Modulus 1.55 GPa
225 ksi
ISO 527-2
Domo 1101N Polypropylene Homopolymer
Information provided by Domo.
Tensile Modulus 1.55 GPa
225 ksi
BASF Novolen® 2248 TC Polypropylene
Nucleated grade with antistatic agent for injection moldings.Data was collected by ISO methods and provided by BASF.
Tensile Modulus 1.55 GPa
225 ksi
1 mm/min
Arkema Group Orgalloy® LE 60HM Flexible Nylon Alloy (Conditioned)
LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents).higher in rigidity than LE 6000. For film, hollow vessel blow moldi..
Tensile Modulus 1.55 GPa
225 ksi
ISO 527-2
Ascend Performance Materials Vydyne® 25WSP Nylon 66, Conditioned (2.5% Moisture)
Vydyne® 25WSP is a black, weather resistant injection molding grade Nylon 66 resin. These resins offer a well-balanced combination of engineering properties characterized by high strength, rigidity..
Tensile Modulus 1.55 GPa
225 ksi
1mm/min; ISO 527
BASF Ultraform N 2640 Z4 BK140 Q600 POM
Ultraform N2640 Z4 BK140 Q600 is a high toughness, elastomer-modified injection molding POM grade.
Tensile Modulus 1.55 GPa
225 ksi
ISO 527
Ascend Performance Materials Vydyne® 22WSP Nylon 66, Weather Resistant, Conditioned
Vydyne® 25WSP is a black, weather resistant injection molding grade Nylon 66 resin. These resins offer a well-balanced combination of engineering properties characterized by high strength, rigidity..
Tensile Modulus 1.55 GPa
225 ksi
BASF Novolen® 1100 N Polypropylene, Injection Molding Grade
Grade for injection molded parts. Also available as a special grade for fibers (short spinning) and cast film.Data was collected by ISO methods and provided by BASF.
Tensile Modulus 1.55 GPa
225 ksi
BASF Novolen® 1148 TC Polypropylene
Nucleated grade with antistatic agent for injection molded parts.Data was collected by ISO methods and provided by BASF.
Tensile Modulus 1.55 GPa
225 ksi
DIN 53457
Isoflon PA 11 Polyamide 11
General use for mechanical partsGood heat resistanceEasy to useInformation provided by Isoflon.
Tensile Modulus 1.55 GPa
225 ksi
roll stack films TD; ISO 527-3
Borealis Bormod™ HC904CF Polypropylene
Bormod™ BJ368MO is a polypropylene copolymer characterized by good flow, and optimum combination of high stiffness and high impact strength. The material is nucleated with Borstar® Nucleation Tech..