| Category | Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, 20% Glass Fiber Reinforced |
| Manufacturer | EMS-Grivory (EMS-CHEMIE) |
| Trade Name | Grivory® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | EMS-Grivory Grivory® HT2VZ-15H PA6T/66-GF15.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.24 g/cc | 0.0448 lb/in³ | ISO 1183 |
| Water Absorption | 5.5 % | 5.5 % | ISO 62 |
| Moisture Absorption | 2.00 % | 2.00 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0040 cm/cm | 0.0040 in/in | ISO 294-4, 2577 |
| Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | ISO 294-4, 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 82 | 82 | conditioned, 15s; ISO 868 |
| 84 | 84 | dry, 15s; ISO 868 | |
| Tensile Strength at Break | 100 MPa | 14500 psi | conditioned; ISO 527-1/-2 |
| 125 MPa | 18100 psi | dry; ISO 527-1/-2 | |
| Elongation at Break | 3.0 % | 3.0 % | dry; ISO 527-1/-2 |
| 3.5 % | 3.5 % | conditioned; ISO 527-1/-2 | |
| Tensile Modulus | 6.00 GPa | 870 ksi | conditioned; ISO 527-1/-2 |
| 6.00 GPa | 870 ksi | dry; ISO 527-1/-2 | |
| Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | conditioned; ISO 179/1eU |
| 6.50 J/cm² | 30.9 ft-lb/in² | dry; ISO 179/1eU | |
| 4.00 J/cm² @Temperature 30.0 °C |
19.0 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU | |
| 4.50 J/cm² @Temperature 30.0 °C |
21.4 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU | |
| Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | dry; ISO 179/1eA |
| 1.00 J/cm² | 4.76 ft-lb/in² | conditioned; ISO 179/1eA | |
| 0.500 J/cm² @Temperature 30.0 °C |
2.38 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU | |
| 0.500 J/cm² @Temperature 30.0 °C |
2.38 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 30.0 µm/m-°C | 16.7 µin/in-°F | ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 75.0 µm/m-°C | 41.7 µin/in-°F | ISO 11359-1/-2 |
| Melting Point | 310 °C | 590 °F | 10°C/min; ISO 11357-1/-3 |
| Maximum Service Temperature, Air | 140 °C | 284 °F | long term; EMS |
| 240 °C | 464 °F | short term; EMS | |
| Deflection Temperature at 1.8 MPa (264 psi) | 265 °C | 509 °F | ISO 75-1/-2 |
| Deflection Temperature at 8.0 MPa | 100 °C | 212 °F | ISO 75-1/-2 |
| Flammability, UL94 | HB | HB | IEC 60695-11-10 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | dry; IEC 60093 |
| 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | conditioned; IEC 60093 | |
| Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
| Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
| 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 | |
| Comparative Tracking Index | 575 V | 575 V | conditioned; IEC 60112 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Automotive | Air intake sytems | |
| Compressed air systems | ||
| Fuel systems | ||
| Hydraulic systems | ||
| Interior | ||
| Powertrain and Chassis | ||
| Electricals & Electronics | Connectors | |
| Electrical appliances | ||
| Electrical equipment | ||
| Energy distribution | ||
| Mobile phones and other portable devices | ||
| Form | Granules | |
| Industry & Consumer goods | Hydraulics & Pneumatics | |
| Mechanical Engineering | ||
| Power transmission | ||
| Tools & Accessories | ||
| Processing | Injection Molding | |
| Product Attributes | Co Polyamide | |
| Improved alcohol resistance | ||
| Partially aromatic Polyamide | ||
| Special Characteristics | High impact or impact modified | |
| Improved heat resistance |