Polymer Property : Maximum Service Temperature, Air = 230 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 - 110 °C
212 - 230 °F
Heat distortion temperature
Abatron AboWeld 55-25/AboCure 55-25 Epoxy  (discontinued **)
Data provided by the manufacturer, Abatron, Inc. Paste form, Modified for minimum shrinkage and better heat transfer. Custom colors. Shelf life is 12+ months.Processing: 1/1 ratio. Pot life: 1-2 ..
Maximum Service Temperature, Air 100 - 110 °C
212 - 230 °F
Heat distortion temperature
Abatron AboWeld 7801-5/AboCure 7801-5 Epoxy  (discontinued **)
Data provided by the manufacturer, Abatron, Inc. Aluminum filled thixotropic paste. The most versatile of metal-filled pastes. Shelf life is 12+ months.Processing: Pot life: 1-2 hrs. 2/1 ratio. Li..
Maximum Service Temperature, Air 100 - 110 °C
212 - 230 °F
Heat distortion temperature
Abatron AboWeld 8012-5/AboCure 8012-5 Epoxy  (discontinued **)
Data provided by the manufacturer, Abatron, Inc. Aluminum filled putty, "plastic aluminum". non-shrinking, tough adhesive filler. Shelf life is 12+ months.Processing: Pot life: 1-2 hrs. 2/1 ratio...
Maximum Service Temperature, Air 100 - 110 °C
212 - 230 °F
Heat distortion temperature
Abatron AboWeld 8012-6/AboCure 8012-6 Epoxy  (discontinued **)
Data provided by the manufacturer, Abatron, Inc. Iron filled putty, "plastic steel". non-shrinking, adhesive filler. Shelf life is 12+ months.Processing: Pot life: 1-2 hrs. 2/1 ratio.Applications:..
Maximum Service Temperature, Air 100 - 110 °C
212 - 230 °F
Softening Range
Huntsman HT 9690 Special Hardener
Mix Ratio with ECN 1299 is 50.Comments/Applications: 0-cresol novolac hardener. *Mix ratio with ECN 1299. Latent with ECN resins. High temperature resistant. Molding compound and powder coatin..
Maximum Service Temperature, Air 90.0 - 110 °C
194 - 230 °F
long term; EMS
EMS-Grivory Grivory® 1SBVX-50H LDS black PA1010-GF50
Product Description: Grilamid 1SBVX-50H LDS black is a 50% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is specifically optimized for the laser Direct Structuring techno..
Maximum Service Temperature, Air 80.0 - 110 °C
176 - 230 °F
long term; EMS
EMS-Grivory Grivory® 2D 25 W 20 HL X black 9992 PA612-I
Product Description: Grilamid 2D 25 W 20 HL X black 9992 is a semi-flexible high viscosity, plasticized, high impact and highly heat resistant polyamide 612 (PA612) grade. Unique properties of Gril..
Maximum Service Temperature, Air 100 - 110 °C
212 - 230 °F
long term; EMS
EMS-Grivory Grivory® 2SV-30H nat PA610-GF30
Product Description: GRILAMID XE3976 natural 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mat..
Maximum Service Temperature, Air 90.0 - 110 °C
194 - 230 °F
long term; EMS
EMS-Grivory Grivory® AG-30 LF 15 PA66-(GF+Z)45
Product description: Grilon AG-30 LF 15 black 9832 is a heat stabilized, normal viscosity PA66 injection molding grade with 30% glass fibers and 15% of a combination of PTFE and silicone. Grilon AG-..
Maximum Service Temperature, Air 90.0 - 110 °C
194 - 230 °F
long term; EMS
EMS-Grivory Grivory® AS V0 PA66
Product description: Grilon AS V0 is an unreinforced, normal viscosity, self-extinguishing PA66 injection molding grade. Grilon AS V0 has the following important properties: Halogen and phosphorous-..
Maximum Service Temperature, Air 90.0 - 110 °C
194 - 230 °F
long term; EMS
EMS-Grivory Grivory® AZ 3 PA66
Product description: Grilon AZ 3 is a normal viscosity, high impact modified PA66 injection molding grade. Grilon AZ 3 has the following important properties: Excellent toughness at low temperatures..
Maximum Service Temperature, Air 80.0 - 110 °C
176 - 230 °F
long term; EMS
EMS-Grivory Grivory® BG-25 HM PA6-GF25
Product description: Grilon BG-25 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 25% glass fibers. Grilon BG-25 HM has the following important prop..
Maximum Service Temperature, Air 80.0 - 110 °C
176 - 230 °F
long term; EMS
EMS-Grivory Grivory® BRZ 247 W PA6
Product description: Grilon BRZ 247 W is a heat stabilized, high viscosity, impact modified and plasticized PA6 extrusion grade. Grilon BRZ 247 W has the following important properties: High flexibi..
Maximum Service Temperature, Air 90.0 - 110 °C
194 - 230 °F
long term; EMS
EMS-Grivory Grivory® L 16 LM PA12
Product Description: Grilamid L 16 LM is a , low viscosity extrusion type, based on Polyamide 12 (PA12). Grilamid L 16 LM is UV- and heat stabilized. The modification with a nucleation agent results..
Maximum Service Temperature, Air 80.0 - 110 °C
176 - 230 °F
long term; EMS
EMS-Grivory Grivory® L 16 W 20 black 9995 PA12
Product Description: Grilamid L 16 W 20 is a semi-flexible low viscosity, heat stabilized PA12 injection molding grade. The main characteristics of this product are: Easy flowing?High impact streng..
Maximum Service Temperature, Air 90.0 - 110 °C
194 - 230 °F
long term; EMS
EMS-Grivory Grivory® L 20 G HL PA12
Product Description: Grilamid L 20 GHL is a, medium viscosity injection molding grade, based on Polyamide 12 (PA12). Grilamid L 20 GHL is UV-stabilized, and heat stabilized The special features of G..
Maximum Service Temperature, Air 90.0 - 110 °C
194 - 230 °F
long term; EMS
EMS-Grivory Grivory® L 20 H FR PA12 FR
Product Description: Grilamid L 20 H FR is a flame retarded, medium viscosity product, based on Polyamide 12 (PA12). Grilamid L 20 H FR contains no halogen or phosphorus, it has a light natural colo..
Maximum Service Temperature, Air 90.0 - 110 °C
194 - 230 °F
long term; EMS
EMS-Grivory Grivory® L 20 LF grey PA12
Product Description: Grilamid L 20 LF grey is a medium viscosity graphite filled Polyamide 12 (PA12) grade suitable for both injection molding and extrusion applications. Grilamid L 20 LF grey has b..
Maximum Service Temperature, Air 90.0 - 110 °C
194 - 230 °F
long term; EMS
EMS-Grivory Grivory® L 20A Z PA12
Product Description: Grilamid L 20A Z is a medium viscosity product, based on Polyamide 12 (PA12). Grilamid L 20A Z is impact modified, hydrolysis-and heat stabilized. Grilamid L 20A Z is used for p..
Maximum Service Temperature, Air 90.0 - 110 °C
194 - 230 °F
long term; EMS
EMS-Grivory Grivory® TSG-25/4 PA666-GF25
Information provided by EMS Grivory
Maximum Service Temperature, Air 90.0 - 110 °C
194 - 230 °F
long term; EMS
EMS-Grivory Grivory® TSG-30/4 FA PA666-GF30
Information provided by EMS Grivory
Maximum Service Temperature, Air 90.0 - 110 °C
194 - 230 °F
long term; EMS
EMS-Grivory Grivory® TSG-30/4 LF 15 PA666-(GF+Z)45
Product description: Grilon TSG-30/4 LF 15 natural is a normal viscosity, heat stabilized PA 66 + PA 6- molding type with 30% glass fibre reinforcement and 15% of a combination PTFE and siliconoil. ..
Maximum Service Temperature, Air 80.0 - 110 °C
176 - 230 °F
long term; EMS
EMS-Grivory Grivory® TSS PA666
Product description: Grilon TSS is an unreinforced, heat stabilized, normal viscosity PA66 + PA6 injection molding grade. Grilon TSS has the following important properties: Excellent flow behaviorHi..
Maximum Service Temperature, Air 90.0 - 110 °C
194 - 230 °F
long term; EMS
EMS-Grivory Grivory® L 25 LM PA12
Product Description: Grilamid L 25 LM is a heat and UV stabilized nylon 12 grade for tube extrusion. According to DIN 73378 Grilamid L 25 LM corresponds to the type PA 12 HL. Grilamid L 25 LM fulfil..
Maximum Service Temperature, Air 80.0 - 110 °C
176 - 230 °F
long term; EMS
EMS-Grivory Grivory® L 25 W 20 X PA12-I
Product Description: Grilamid L 25 W 20 X is a semi-flexible plasticized high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 20 X is impact modified and UV and heat stabilized. Th..
Maximum Service Temperature, Air 80.0 - 110 °C
176 - 230 °F
long term; EMS
EMS-Grivory Grivory® L 25 W 40 HL X PA12-I
Product Description: Grilamid L 25 W 40 HLX is a flexible Polyamide 12 grade with an excellent cold impact strength and heat stability. Grilamid L 25 W 40 HLX is specially suitable for flexible tube..
Maximum Service Temperature, Air 80.0 - 110 °C
176 - 230 °F
long term; EMS
EMS-Grivory Grivory® TRV-4X9 PAMACM12-GF40
Product description: Grilamid TRV-4X9 is an amorphous, cycloaliphatic polyamide with 40% glass fibre reinforcement. Grilamid TRV-4X9 characterises itself through the following features: Very low shr..
Maximum Service Temperature, Air 100 - 110 °C
212 - 230 °F
Heat distortion temperature
Abatron AboCast 50-3/AboCure 50-1 Epoxy
Data provided by the manufacturer, Abatron, Inc. Honey viscosity, light amber color. Best combination of high strength and versatility for Abatron "VR" Epoxies. Shelf life is 12+ months.Processin..
Maximum Service Temperature, Air 90.0 - 110 °C
194 - 230 °F
long term; EMS
EMS-Grivory Grivory® BM-30/2 PA6-MD30
Product description: Grilon BM-30/2 is a 30% mineral reinforced PA6 injection molding grade. Grilon BM-30/2 has the following important properties: Iow warpageImpact resistantIsotropic shrinkage App..
Maximum Service Temperature, Air 80.0 - 110 °C
176 - 230 °F
long term; EMS
EMS-Grivory Grivory® TRVX-50X9 nat PAMACM12-GF50
Product description: Grilamid TRVX-50X9 is a 50% glass fiber reinforced amorphous polyamide. This product shows a very low tendency of distortion and is therefore especially suitable for complex and..