| Category | Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC) |
| Manufacturer | Techmer ES |
| Trade Name | Plastiblend® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Techmer ES Plastiblend® PC/ABS FR 6206.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.16 g/cc | 0.0419 lb/in³ | ASTM D792 |
| Water Absorption | 0.10 % <br>@Time 86400 sec |
0.10 % <br>@Time 24.0 hour |
ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0050 cm/cm <br>@Thickness 3.17 mm |
0.0050 in/in <br>@Thickness 0.125 in |
ASTM D955 |
| Melt Flow | 19 g/10 min <br>@Load 2.16 kg,<br> Temperature 260 °C |
19 g/10 min <br>@Load 4.76 lb,<br> Temperature 500 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 120 | 120 | ASTM D785 |
| Tensile Strength, Yield | 56.5 MPa | 8200 psi | ASTM D638 |
| Elongation at Break | 50 % | 50 % | ASTM D638 |
| Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
| Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
| Izod Impact, Notched | 1.60 J/cm <br>@Thickness 3.17 mm,<br> Temperature -28.9 °C |
3.00 ft-lb/in <br>@Thickness 0.125 in,<br> Temperature -20.0 °F |
ASTM D256 |
| 4.27 J/cm <br>@Thickness 3.17 mm,<br> Temperature 22.8 °C |
8.00 ft-lb/in <br>@Thickness 0.125 in,<br> Temperature 73.0 °F |
ASTM D256 | |
| Dart Drop, Total Energy | 53.1 J <br>@Temperature -28.9 °C |
39.2 ft-lb <br>@Temperature -20.0 °F |
ASTM D3763 |
| 58.7 J <br>@Temperature 22.8 °C |
43.3 ft-lb <br>@Temperature 73.0 °F |
ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 72.0 µm/m-°C | 40.0 µin/in-°F | ASTM D696 |
| Deflection Temperature at 1.8 MPa (264 psi) | 73.9 °C | 165 °F | Unannealed; ASTM D648 |
| Flammability, UL94 | V-0 <br>@Thickness 1.50 mm |
V-0 <br>@Thickness 0.0590 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+18 ohm-cm | 1.00e+18 ohm-cm | ASTM D257 |