Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Paxon™ AA60-003 Blow Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Exxon Chemical
Trade Name Paxon™
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF ExxonMobil Paxon™ AA60-003 Blow Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: AA60-003 is a medium molecular weight distribution high density polyethylene which is characterized by high stiffness, excellent melt uniformity, and chemical inertness.Availability: Latin America, North America and South America Additive: Thermal Stabilizer: YesAntistatic: No Applications: Food packagingLiquid Food Containers for Milk, Water and JuicesThermoformed PartsThin Gauge SheetInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.963 g/cc
0.0348 lb/in³
ASTM D4883
ESCR 100% Igepal® 20 hour
20 hour
ASTM D1693 Condition B
Melt Flow 0.25 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.25 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.7 MPa
4600 psi
ASTM D638
Elongation at Break 450 %
450 %
ASTM D638
Flexural Modulus 1.62 GPa
235 ksi
Method1, Procedure A (1"x3"x0.125"), Tangent calculation; ASTM D790
Tensile Impact Strength 147 kJ/m²
70.0 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
Vicat Softening Point 127 °C
260 °F
ASTM D1525
Brittleness Temperature <= -76.1 °C
<= -105 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 191 °C
375 °F
Users viewing this material also viewed the following: