| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 220 °C | 428 °F | Continuous |
|
Pyrotek TS-106 Thermoset Electrical Insulation Product
Glass reinforcement, Polyester resin, Tan / Red color. High heat resistance. UL recognized.Information provided by Pyrotek.
|
|||
| Maximum Service Temperature, Air | 220 °C | 428 °F | Continuous |
|
Quadrant EPP Techtron® HPV PPS + solid lubricant, bearing grade, extruded (ISO Data)
As a reinforced, internally lubricated PPS grade, Techtron HPV PPS demonstrates an excellent combination of properties including wear resistance, load-bearing capabilities and dimensional stability ..
|
|||
| Maximum Service Temperature, Air | 220 °C | 428 °F | Short Time; IEC 60216 |
|
PolyOne Bergamid™ A70 G25 H natur TM-X Polyamide 66 (Nylon 66)
Information provided by PolyOne
|
|||
| Maximum Service Temperature, Air | 220 °C | 428 °F | ASTM D794 |
|
Solvay Specialty Polymers Primef® 7002 Polyphenylene Sulfide (PPS), 65% GlassMineral
(discontinued **)
Primef 7002 is a 65% mineral/glass fiber reinforced polyphenylene sulfide (PPS). This grade offers higher fluidity than Primef 7010 (also 65% mineral/glass fiber), but with somewhat lower mechanical..
|
|||
| Maximum Service Temperature, Air | 220 - 240 °C | 428 - 464 °F | Average value: 230 °C Grade Count:4 |
|
Overview of materials for Polyphenylene Sulfide (PPS), Aramid Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Aramid Fiber". Each property range of values reported is minimum and maximu..
|
|||
| Maximum Service Temperature, Air | 220 °C | 428 °F | |
|
Lehmann & Voss LUVOCOM® 1301-0793 PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. ..
|
|||
| Maximum Service Temperature, Air | 220 °C | 428 °F | |
|
Lehmann & Voss LUVOCOM® 1301-7661/RD PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved fr..
|
|||
| Maximum Service Temperature, Air | 220 °C | 428 °F | short term |
|
Lehmann & Voss LUVOCOM® 1301-8367 PPS, linear, with CNT
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. ..
|
|||
| Maximum Service Temperature, Air | 220 °C | 428 °F | |
|
Greene Tweed CHEMRAZ® 565 Perfluoroelastomer
Chemraz®, a proprietary Greene, Tweed compound, has the broadest chemical resistance of any elastomeric material. Chemraz combines the resilience and sealing force of an elastomer with chemical r..
|
|||
| Maximum Service Temperature, Air | 220 °C | 428 °F | Resistance to heat - ball pressure test; IEC 60695-10-2 |
|
Lanxess Pocan® T 7391 POS151 900044 PBT + PET, 45% Glass Fiber
PBT + PET, 45% glass fibers, injection molding, improved surface finish, increased temperature peak load UV stabilizedInformation provided by LANXESS.
|
|||
| Maximum Service Temperature, Air | 220 °C | 428 °F | short term |
|
Lehmann & Voss LUVOCOM® 1100-7721/WT9016 Polyether sulfone, unreinforced
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
|
|||
| Maximum Service Temperature, Air | 220 °C | 428 °F | Short peaks operation |
|
Polyram PlusTek PA350M6 Nylon 6.6 for Injection Molding, 30% Mineral Reinforced
30% Minerals Reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram.
|
|||
| Maximum Service Temperature, Air | 220 °C | 428 °F | short term; EMS |
|
EMS-Grivory Grivory® AZ 3/2 PA66
Product description: Grilon AZ 3/2 is an unreinforced and impact modified PA66 injection molding grade. Grilon AZ 3/2 has the following important properties: Excellent toughness at low temperaturesE..
|
|||
| Maximum Service Temperature, Air | 220 °C | 428 °F | short term; EMS |
|
EMS-Grivory Grivory® GV XE 16101 (GVL-5H HP) PA*-GF50
Product description: Grivory XE 16101 natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long special glass fibers. Grivory..
|
|||
| Maximum Service Temperature, Air | 220 °C | 428 °F | short term; EMS |
|
EMS-Grivory Grivory® GV-5H EF nat PA*-GF50
Product description: Grivory GV-5H EF natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyam..
|
|||
| Maximum Service Temperature, Air | 220 °C | 428 °F | short term; EMS |
|
EMS-Grivory Grivory® GV-6 FWA nat PA*-GF60
Product description: Grivory GV-6 FWA natural is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami..
|
|||
| Maximum Service Temperature, Air | 220 °C | 428 °F | short term; EMS |
|
EMS-Grivory Grivory® GVL-5H black 9839 PA*-GF50
Product description: Grivory GVL-5H black 9839 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H..
|
|||
| Maximum Service Temperature, Air | 220 °C | 428 °F | short term; EMS |
|
EMS-Grivory Grivory® GVX-65 H black 9915 PA*-GF65
Product description: Grivory GVX-65H black 9915 is a 65% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolya..
|
|||
| Maximum Service Temperature, Air | 220 °C | 428 °F | 220°C insulation by UL, the US Navy, and other tests |
|
DuPont™ Nomex® 410 Paper, 25.5 mil Nominal Thickness
Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is ..
|
|||
| Maximum Service Temperature, Air | 220 °C | 428 °F | Electrical insulation |
|
DuPont™ Nomex® 414 Paper, 7 mil Nominal Thickness
Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand..
|
|||
| Maximum Service Temperature, Air | 220 °C | 428 °F | DuPont Test Method |
|
DuPont Performance Polymers Kalrez® Spectrum™ 0040 Fluoroelastomer
Kalrez® Spectrum™ 0040 perfluoroelastomer parts are specifically designed for low-temperature environments where significant chemical resistance is required. Proprietary polymer and cure technolog..
|
|||
| Maximum Service Temperature, Air | 220 °C | 428 °F | short term; EMS |
|
EMS-Grivory Grivory® GVL-5H black 9915 PA*-GF50
Product description: Grivory GVL-5H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H blac..
|
|||
| Maximum Service Temperature, Air | 220 °C | 428 °F | short term; EMS |
|
EMS-Grivory Grivory® GVX-6 H black 9915 PA*-GF60
Product description: Grivory GVX-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam..
|
|||
| Maximum Service Temperature, Air | 220 °C | 428 °F | rated per UL Card E54153 |
|
Arlon 55609R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Uncured Silicone RubberProduct Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThi..
|
|||
| Maximum Service Temperature, Air | 220 °C | 428 °F | |
|
3M Dyneon™ TFE 90Z Peroxide Cure Perfluoroelastomer
3M™ Dyneon™ Peroxide Cure Perfluoroelastomer PFE 90Z is a technically advanced peroxide curable perfluoroelastomer, designed to meet the challenges of demanding sealing applications. It is classif..
|
|||
| Maximum Service Temperature, Air | 220 °C | 428 °F | short term; EMS |
|
EMS-Grivory Grivory® GV-4H black PA*-GF40
Product description: Grivory GV-4H black 9915 is a 40% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami..
|
|||
| Maximum Service Temperature, Air | 220 °C | 428 °F | short term; EMS |
|
EMS-Grivory Grivory® GV-6H EF nat PA*-GF60
Product description: Grivory GV-6H EF black 9915 is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol..
|
|||
| Maximum Service Temperature, Air | 220 °C | 428 °F | Pigment Heat Resistance; EN 12877-3 |
|
Karina 06/706-RG-GE (CS) Blue Color Concentrate for PVC
Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. ..
|
|||
| Maximum Service Temperature, Air | 220 °C | 428 °F | |
|
LATI Laticonther 80 GR/50 PPS, 50% Graphite Reinforced
High thermal conductivity product based on Polyphenylene Sulfide (PPS). Graphite. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
|
|||