Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Delrin® 100PE BK602 Acetal (POM)  (Unverified Data**)

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Homopolymer, Unreinforced
Manufacturer DuPont Performance Polymers
Trade Name Delrin®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Delrin® 100PE BK602 Acetal (POM)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100PE BK602 (formerly DE20573) is a high viscosity acetal homopolymer an enhanced version of Delrin 100P with very low VOC emissions. It has a great combination of strength and toughnessInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
1.42 g/cc
0.0513 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.022 cm/cm
0.022 in/in
ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ISO 294-4 2577
Melt Flow 2.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
cm³/10min; ISO 1133
2.6 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.6 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell M 92
92
ISO 2039-2
Hardness, Rockwell R 120
120
ISO 2039-2
Tensile Strength, Yield 72.0 MPa
10400 psi
ISO 527-1/-2
Elongation at Break 32 %
32 %
Nominal; ISO 527-1/-2
Elongation at Yield 21 %
21 %
ISO 527-1/-2
Tensile Modulus 3.10 GPa
450 ksi
ISO 527-1/-2
Flexural Strength 80.0 MPa

@Strain 3.50 %
11600 psi

@Strain 3.50 %
ISO 178
Flexural Modulus 2.90 GPa
421 ksi
ISO 178
Charpy Impact Unnotched 35.0 J/cm²
167 ft-lb/in²
ISO 179/1eU
30.0 J/cm²

@Temperature -30.0 °C
143 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²
5.23 ft-lb/in²
ISO 179/1eA
1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 110 µm/m-°C
61.1 µin/in-°F
ISO 11359-1/-2
100 µm/m-°C

@Temperature -40.0 - 23.0 °C
55.6 µin/in-°F

@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 110 µm/m-°C
61.1 µin/in-°F
ISO 11359-1/-2
100 µm/m-°C

@Temperature -40.0 - 23.0 °C
55.6 µin/in-°F

@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 97.0 °C
207 °F
ISO 75-1/-2
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
IEC 60093
Surface Resistance 5.00e+13 ohm
5.00e+13 ohm
IEC 60093
Dielectric Constant 3.9

@Frequency 100 Hz
3.9

@Frequency 100 Hz
IEC 60250
3.9

@Frequency 1.00e+6 Hz
3.9

@Frequency 1.00e+6 Hz
IEC 60250
Dielectric Strength 44.0 kV/mm
1120 kV/in
IEC 60243-1
Dissipation Factor 0.00050

@Frequency 100 Hz
0.00050

@Frequency 100 Hz
IEC 60250
0.0055

@Frequency 1.00e+6 Hz
0.0055

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Descriptive Properties Value Comments
Additives Release agent
Delivery Form Pellets
Emissions <2 mg/kg
VDA 275
Part Marking Code >POM<
ISO 11469
Processing Injection Moulding
Other Extrusion
Profile Extrusion
Sheet Extrusion
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification POM
ISO 1043
Users viewing this material also viewed the following: