Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Stanyl® OCD2100 BK27021 PA46-GF40

Category Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Glass Fiber Reinforced
Manufacturer DSM Engineering Plastics
Trade Name Stanyl®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF DSM Stanyl® OCD2100 BK27021 PA46-GF40.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
40% Glass Reinforced, Heat Stabilized
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
dry; ISO 1183
Moisture Absorption 2.20 %
2.20 %
Sim. To ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm
0.0050 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm
0.010 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 125 MPa
18100 psi
cond; ISO 527-1/-2
210 MPa
30500 psi
dry; ISO 527-1/-2
60.0 MPa

@Temperature 200 °C
8700 psi

@Temperature 392 °F
ISO 527-1/-2
75.0 MPa

@Temperature 180 °C
10900 psi

@Temperature 356 °F
ISO 527-1/-2
85.0 MPa

@Temperature 160 °C
12300 psi

@Temperature 320 °F
ISO 527-1/-2
100 MPa

@Temperature 120 °C
14500 psi

@Temperature 248 °F
ISO 527-1/-2
Elongation at Break 3.0 %
3.0 %
dry; ISO 527-1/-2
8.0 %
8.0 %
cond; ISO 527-1/-2
10 %

@Temperature 120 °C
10 %

@Temperature 248 °F
ISO 527-1/-2
11 %

@Temperature 160 °C
11 %

@Temperature 320 °F
ISO 527-1/-2
12 %

@Temperature 180 °C
12 %

@Temperature 356 °F
ISO 527-1/-2
12.5 %

@Temperature 200 °C
12.5 %

@Temperature 392 °F
ISO 527-1/-2
Tensile Modulus 7.00 GPa
1020 ksi
cond; ISO 527-1/-2
13.0 GPa
1890 ksi
dry; ISO 527-1/-2
3.40 GPa

@Temperature 200 °C
493 ksi

@Temperature 392 °F
ISO 527-1/-2
4.20 GPa

@Temperature 180 °C
609 ksi

@Temperature 356 °F
ISO 527-1/-2
4.60 GPa

@Temperature 160 °C
667 ksi

@Temperature 320 °F
ISO 527-1/-2
5.00 GPa

@Temperature 120 °C
725 ksi

@Temperature 248 °F
ISO 527-1/-2
Flexural Modulus 7.00 GPa
1020 ksi
cond; ISO 178
13.0 GPa
1890 ksi
dry; ISO 178
3.40 GPa

@Temperature 200 °C
493 ksi

@Temperature 392 °F
ISO 178
4.20 GPa

@Temperature 180 °C
609 ksi

@Temperature 356 °F
ISO 178
4.60 GPa

@Temperature 160 °C
667 ksi

@Temperature 320 °F
ISO 178
5.00 GPa

@Temperature 120 °C
725 ksi

@Temperature 248 °F
ISO 178
Izod Impact Resistance 1.50 J/cm²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 180/1A
2.50 J/cm²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
cond; ISO 180/1A
Charpy Impact Unnotched 6.50 J/cm²

@Temperature -30.0 °C
30.9 ft-lb/in²

@Temperature -22.0 °F
dry; ISO 179/1eU
7.50 J/cm²

@Temperature -30.0 °C
35.7 ft-lb/in²

@Temperature -22.0 °F
cond; ISO 179/1eU
9.00 J/cm²

@Temperature 23.0 °C
42.8 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eU
10.5 J/cm²

@Temperature 23.0 °C
50.0 ft-lb/in²

@Temperature 73.4 °F
cond; ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²

@Temperature -30.0 °C
5.71 ft-lb/in²

@Temperature -22.0 °F
cond; ISO 179/1eA
1.20 J/cm²

@Temperature -30.0 °C
5.71 ft-lb/in²

@Temperature -22.0 °F
dry; ISO 179/1eA
1.50 J/cm²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eA
2.50 J/cm²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
cond; ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 25.0 µm/m-°C
13.9 µin/in-°F
dry; ISO 11359-1/-2
CTE, linear, Transverse to Flow 50.0 µm/m-°C
27.8 µin/in-°F
dry; ISO 11359-1/-2
Melting Point 282 °C
540 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 256 °C
493 °F
dry; ISO 75-1/-2
Electrical Properties Metric English Comments
Comparative Tracking Index 300 V
300 V
dry; IEC 60112
Users viewing this material also viewed the following: