| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.0040 cm/cm | 0.0040 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
| Elongation at Break | 6.0 % | 6.0 % | ASTM D638 |
| Elongation at Yield | 6.0 % | 6.0 % | ASTM D638 |
| Flexural Yield Strength | 75.8 MPa | 11000 psi | ASTM D790 |
| Flexural Modulus | 6.07 GPa | 880 ksi | ASTM D790 |
| Izod Impact, Notched | 0.534 J/cm @Temperature 22.8 °C |
1.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 103 °C | 217 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 96.1 °C | 205 °F | ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 210 - 238 °C | 410 - 460 °F | |
| Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
| Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
| 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial | |
| Back Pressure | 0.345 - 1.72 MPa | 50.0 - 250 psi | |
| Shot Size | 30 - 80 % | 30 - 80 % | |
| Screw Speed | 20 - 100 rpm | 20 - 100 rpm |