CTC X-PRO CTC PP 2015 Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer CTC (Composite Technologies)
Trade Name X-PRO
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CTC X-PRO CTC PP 2015 Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
X-PRO PP 2015 is an impact, polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC).
Physical Properties Metric English Comments
Melt Flow 15 g/10 min
15 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.1 MPa
3500 psi
ISO 527-1/2
Flexural Modulus 0.827 GPa
120 ksi
0.05 in/min; ISO 178
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ISO 180/A
Processing Properties Metric English Comments
Rear Barrel Temperature 182 - 216 °C
360 - 420 °F
Middle Barrel Temperature 193 - 227 °C
380 - 440 °F
Front Barrel Temperature 204 - 216 °C
400 - 420 °F
Nozzle Temperature 204 - 216 °C
400 - 420 °F
Melt Temperature 204 - 227 °C
400 - 440 °F
Mold Temperature 26.7 - 60.0 °C
80.0 - 140 °F
Back Pressure 0.345 - 1.03 MPa
50.0 - 150 psi
Clamp Pressure 27.6 - 34.5 MPa
4000 - 5000 psi
Descriptive Properties Value Comments
Boost Pressure (psi) 500-1500
Color General Purpose Black
Hold Pressure 50 - 75% of Boost
Screw Speed Medium to Fast