| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.35 g/cc | 0.0488 lb/in³ | ISO 1183 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 145 MPa | 21000 psi | ISO 527 |
| Elongation at Break | 2.4 % | 2.4 % | ISO 527 |
| Flexural Modulus | 7.90 GPa | 1150 ksi | ISO 178 |
| Izod Impact, Notched (ISO) | 7.70 kJ/m² | 3.66 ft-lb/in² | ISO 180 |
| Charpy Impact, Notched | 0.850 J/cm² | 4.04 ft-lb/in² | ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 245 °C | 473 °F | ISO 75 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 285 - 300 °C | 545 - 572 °F | |
| Mold Temperature | 80.0 - 90.0 °C | 176 - 194 °F | |
| Dry Time | 2 - 4 hour | 2 - 4 hour | |
| Moisture Content | <= 0.050 % | <= 0.050 % |