| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 61.0 MPa | 8850 psi | 50 mm/min; ISO 527 |
| SABIC Innovative Plastics Cycoloy® CX2142ME PC+ABS (Asia Pacific) Cycoloy* resin grade CX2142ME is an injection moldable PC/ABS blend with Br- and Cl-free flame retardant systems. Key features of good flow, good impact, UL-94 V0 rating at 1.2 mm, and improved chem.. |
|||
| Tensile Strength, Yield | 61.0 MPa | 8850 psi | 5 mm/min; ISO 527 |
| SABIC Innovative Plastics Lexan® FXG154 PC FXG154 is a Lexan PC grade with the Diamond effect. Color Package may affect properties, Application testing always recommended.This data was supplied by SABIC-IP for the Americas region. |
|||
| Tensile Strength, Yield | 61.0 MPa | 8850 psi | 50 mm/min; ISO 527 |
| SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer 55 MFR LEXAN High Flow Ductile Copolymer, Natural color only |
|||
| Tensile Strength, Yield | 61.0 MPa | 8850 psi | 50 mm/min; ISO 527 |
| SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer (Europe-Africa-Middle East) 55 MFR LEXAN High Flow Ductile Copolymer, Natural color only |
|||
| Tensile Strength, Yield | 61.0 MPa | 8850 psi | Type I, 50 mm/min; ASTM D 638 |
| SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer (Asia Pacific) High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E.. |
|||
| Tensile Strength, Yield | 61.0 MPa | 8850 psi | Type I, 50 mm/min; ASTM D 638 |
| SABIC Innovative Plastics Lexan® HPM1944 PC (Asia Pacific) Medium flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). .. |
|||
| Tensile Strength, Yield | 61.0 MPa | 8850 psi | 50 mm/min; ISO 527 |
| SABIC Innovative Plastics Lexan® HPS4 PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).EtO, steam, e-beam, and gamma sterilizable... |
|||
| Tensile Strength, Yield | 61.0 MPa | 8850 psi | 50 mm/min; ISO 527 |
| SABIC Innovative Plastics Lexan® LUX2910 PC (Asia Pacific) Global grade. LEXAN LUX2910 is an injection moulding grade especially designed for manufacturing optical parts requiring superior flow properties combined with very high transmission and color stabi.. |
|||
| Tensile Strength, Yield | 61.0 MPa | 8850 psi | Type I, 50 mm/min; ASTM D638 |
| SABIC Innovative Plastics Lexan® OQ1022 PC Standard Flow OQ Resin |
|||
| Tensile Strength, Yield | 61.0 MPa | 8850 psi | 50 mm/min; ISO 527 |
| SABIC Innovative Plastics Lexan® OQ1022 PC Standard Flow OQ Resin |
|||
| Tensile Strength, Yield | 61.0 MPa | 8850 psi | Type I, 5 mm/min; ASTM D638 |
| SABIC Innovative Plastics LNP COLORCOMP D10006U PC LNP* COLORCOMP* D10006U is an unfilled Polycarbonate. Added features include: Lasermarking Capability, UL Listed. |
|||
| Tensile Strength, Yield | 61.0 MPa | 8850 psi | 50 mm/min; ISO 527 |
| SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer 55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only |
|||
| Tensile Strength, Yield | 61.0 MPa | 8850 psi | 50 mm/min; ISO 527 |
| SABIC Innovative Plastics Lexan® HPS7 PC Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
| Tensile Strength, Yield | 61.0 MPa | 8850 psi | ASTM D638 |
| Global POM-90 General Purpose Acetal Information provided by Global Polymers Corporation. |
|||
| Tensile Strength, Yield | 61.0 MPa | 8850 psi | ASTM D638 |
| SABIC Innovative Plastics LNP STAT-KON DD0009 PC LNP* STAT-KON* DD0009 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
| Tensile Strength, Yield | 61.0 MPa | 8850 psi | Type I, 5 mm/min; ASTM D638 |
| SABIC Innovative Plastics LNP STAT-KON DD0009E PC LNP* STAT-KON* DD0009E is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant, Easy Molding. |
|||
| Tensile Strength, Yield | 61.0 MPa | 8850 psi | Type I, 50 mm/min; ASTM D638 |
| SABIC Innovative Plastics Xenoy® 1731 PBT+PC Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD. |
|||
| Tensile Strength, Yield | 61.0 MPa | 8850 psi | 50 mm/min; ISO 527 |
| SABIC Innovative Plastics Xenoy® X4830 PBT+PC Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
| Tensile Strength, Yield | 61.0 MPa | 8850 psi | Type I, 50 mm/min; ASTM D638 |
| SABIC Innovative Plastics XYLEX X7507 PC+POLYESTER (Europe-Africa-Middle East) F-1 weathering certified in natural color, specially designed for Pool & Spa applications. Currently available in natural color only. |
|||
| Tensile Strength, Yield | 61.0 MPa | 8850 psi | 50mm/min; ISO 527 |
| Teijin Panlite® L-1250Y Standard (mold release/ice color grade) Polycarbonate Resin Standard injection molding grade that has an improved mold release property and is bluish-tinted to exhibit clear color.Applications:Components of mechanical, electric, electronic, medical, safety a.. |
|||
| Tensile Strength, Yield | 61.0 MPa | 8850 psi | 50mm/min; ISO 527 |
| Teijin Panlite® L-1250Z100 Transparent and Weather Resistant grade Polycarbonate Resin Conforms to SAE regulations. It is an injection molding grade that has normal fluidity and weather resistance and is bluish-tinted to exhibit clear color.Applications:Components of mechanical, elect.. |
|||
| Tensile Strength, Yield | 61.0 MPa | 8850 psi | Type I, 5 mm/min; ASTM D 638 |
| SABIC Innovative Plastics Noryl GTX GTX965 PPE+PA66 NORYL GTX965 is a mineral reinforced PPE/PA blend. It offers excellent surface appearance, processability and dimensional stability at elevated temperatures. The best molding condition for good appe.. |
|||
| Tensile Strength, Yield | 61.0 MPa | 8850 psi | 50mm/min; ISO 527 |
| Teijin Panlite® LV-2250Z Transparent and Weather Resistant grade Polycarbonate Resin Typical injection molding grade that has weather resistance and is bluish-tinted to exhibit clear color.Applications:Components of electric, electronic, business machine and industrial equipment com.. |
|||
| Tensile Strength, Yield | 61.0 MPa | 8850 psi | 50 mm/min; ISO 527 |
| SABIC Innovative Plastics NORYL FP6130 PPE+PS (Asia Pacific) Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
| Tensile Strength, Yield | 61.0 MPa | 8850 psi | chs 2.0 in/min; ASTM D638 |
| Diamond Polymers DIAMALOY 173U PC/Polyester Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
| Tensile Strength, Yield | 61.0 MPa | 8850 psi | |
| Asahi Kasei Xyron® AT600 Modified Polyphenylene Ether Applications: Automotive: Body Panels, Mirror Shells, Fuel Door Covers, Hinge Covers, Relay Blocks Electrical and Industrial: Tractor Hoods, Motorcycle Fairings, Yard Maintenance EquipmentInformati.. |
|||
| Tensile Strength, Yield | 61.0 MPa | 8850 psi | ASTM D638 |
| Ashley Polymers Ashlene® R528LW Nylon 66 General purpose injection molding grade Nylon 66, lubricated and FDA approved.Data provided by the manufacturer |
|||
| Tensile Strength, Yield | 61.0 MPa | 8850 psi | 50 mm/min; ISO 527 |
| SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER (Europe-Africa-Middle East) Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts.. |
|||
| Tensile Strength, Yield | 61.0 MPa | 8850 psi | 50 mm/min; ISO 527 |
| SABIC Innovative Plastics Lexan® HP4NR PC (Asia Pacific) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no m.. |
|||