Category | Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber |
Manufacturer | Arlon |
Trade Name | |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Arlon CP-414R Silicone Rubber.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.35 g/cc | 1.35 g/cc | Arlon SQA-TMS-024 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore A | 60 | 60 | ASTM D2240 |
Tensile Strength, Ultimate | 5.52 MPa | 800 psi | ASTM D412 |
Elongation at Break | 225 % | 225 % | ASTM D412 |
Tear Strength | 15.8 kN/m | 90.0 pli | Die B; silicone property; ASTM D624 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 232 °C | 450 °F | |
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
UL RTI, Electrical | 200 °C | 392 °F | |
UL RTI, Mechanical without Impact | 200 °C | 392 °F |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 15.7 kV/mm | 400 kV/in | ASTM D149 |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 120 min @Temperature 204 °C |
2.00 hour @Temperature 400 °F |
|
15.0 min @Pressure 0.345 MPa, Temperature 121 °C |
0.250 hour @Pressure 50.0 psi, Temperature 250 °F |
||
Shelf Life | 6.00 Month @Temperature 23.9 °C |
6.00 Month @Temperature 75.0 °F |
Descriptive Properties | Value | Comments |
---|---|---|
Color | Red |